In situ Nanoindentation Study of Plastic Co-deformation in Al-TiN Nanocomposites

نویسندگان

  • N. Li
  • H. Wang
  • A. Misra
  • J. Wang
چکیده

We performed in situ indentation in a transmission electron microscope on Al-TiN multilayers with individual layer thicknesses of 50 nm, 5 nm and 2.7 nm to explore the effect of length scales on the plastic co-deformability of a metal and a ceramic. At 50 nm, plasticity was confined to the Al layers with easy initiation of cracks in the TiN layers. At 5 nm and below, cracking in TiN was suppressed and post mortem measurements indicated a reduction in layer thickness in both layers. The results demonstrate the profound size effect in enhancing plastic co-deformability in nanoscale metal-ceramic multilayers.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

INVESTIGATION OF TRIBOLOGICAL CHARACTERISTICS OF AL/NANO SiO2NANOCOMPOSITES PRODUCED BY ACCUMULATIVE ROLL BONDING (ARB) PROCESS

Accumulative roll-bonding process (ARB) is an important severe plastic deformation technique for production of the ultrafine grained, nanostructured and nanocomposite materials in the form of plates and sheets. In the present work, this process used for manufacturing Al/SiO 2 nanocomposites by using Aluminum 1050 alloy sheets and nano sized SiO 2 particles, at ambient temperature. After 8 cycle...

متن کامل

Grain Refinement Efficiency of Multi-Axial Incremental Forging and Shearing: A Crystal Plasticity Analysis

Severe plastic deformation is a technical method to produce functional material with special properties such as high strength and specific physical properties. Selection of an efficient severe plastic deformation for grain refinement is a challenging field of study and using a modeling technique to predict the refinement efficiency has gained a lot of attentions. A comparative study was carried...

متن کامل

In situ observation of fracture sequence of physical vapor deposited TiN film on (1120) sapphire

The critical parameters for the structural stability of physical vapor deposited TiN film on (112̄0) sapphire were investigated by analyzing the adhesion strength and failure mechanism through in situ observations of the fracture sequence during scratch tests and static normal indentation. TiN was deposited by arc ion plating on (112̄0) sapphire, and the thickness of the TiN film was controlled t...

متن کامل

Friedel oscillations are limiting the strength of superhard nanocomposites and heterostructures.

To obtain a deeper understanding of the mechanism of plastic deformation and failure in superhard nanocomposites and heterostructures we studied, by means of the ab initio density functional theory, the stress-strain response and the change of the electronic structure during tensile and shear deformation of a prototype interfacial systems consisting of 1 monolayer SiN sandwiched between a few n...

متن کامل

Rate-dependent serrated flow and plastic deformation in Ti45Zr16Be20Cu10Ni9 bulk amorphous alloy during nanoindentation.

The plastic deformation of Ti45Zr16Be20Cu10Ni9 bulk metallic glass has been investigated by nanoindentation performed with loads ranging from 10 to 200 mN in a wide range of loading rates. The plastic flow in the alloy exhibited conspicuous serrations at low loading rates. The serrations, however, became less prominent as the rate of indentation increased. Atomic force microscopy showed a signi...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 4  شماره 

صفحات  -

تاریخ انتشار 2014