Biofilm and Diatom Succession on Polyethylene (PE) and Biodegradable Plastic Bags in Two Marine Habitats: Early Signs of Degradation in the Pelagic and Benthic Zone?
نویسندگان
چکیده
The production of biodegradable plastic is increasing. Given the augmented littering of these products an increasing input into the sea is expected. Previous laboratory experiments have shown that degradation of plastic starts within days to weeks. Little is known about the early composition and activity of biofilms found on biodegradable and conventional plastic debris and its correlation to degradation in the marine environment. In this study we investigated the early formation of biofilms on plastic shopper bags and its consequences for the degradation of plastic. Samples of polyethylene and biodegradable plastic were tested in the Mediterranean Sea for 15 and 33 days. The samples were distributed equally to a shallow benthic (sedimentary seafloor at 6 m water depth) and a pelagic habitat (3 m water depth) to compare the impact of these different environments on fouling and degradation. The amount of biofilm increased on both plastic types and in both habitats. The diatom abundance and diversity differed significantly between the habitats and the plastic types. Diatoms were more abundant on samples from the pelagic zone. We anticipate that specific surface properties of the polymer types induced different biofilm communities on both plastic types. Additionally, different environmental conditions between the benthic and pelagic experimental site such as light intensity and shear forces may have influenced unequal colonisation between these habitats. The oxygen production rate was negative for all samples, indicating that the initial biofilm on marine plastic litter consumes oxygen, regardless of the plastic type or if exposed in the pelagic or the benthic zone. Mechanical tests did not reveal degradation within one month of exposure. However, scanning electron microscopy (SEM) analysis displayed potential signs of degradation on the plastic surface, which differed between both plastic types. This study indicates that the early biofilm formation and composition are affected by the plastic type and habitat. Further, it reveals that already within two weeks biodegradable plastic shows signs of degradation in the benthic and pelagic habitat.
منابع مشابه
Macrofouling communities and the degradation of plastic bags in the sea: an in situ experiment
The increasing amount of plastic littered into the sea may provide a new substratum for benthic organisms. These marine fouling communities on plastic have not received much scientific attention. We present, to our knowledge, the first comprehensive analysis of their macroscopic community composition, their primary production and the polymer degradation comparing conventional polyethylene (PE) ...
متن کاملLaboratory Test Methods to Determine the Degradation of Plastics in Marine Environmental Conditions
In this technology report, three test methods were developed to characterize the degradation of plastic in marine environment. The aim was to outline a test methodology to measure the physical and biological degradation in different habitats where plastic waste can deposit when littered in the sea. Previously, research has focused mainly on the conditions encountered by plastic items when float...
متن کاملBiostratigraphy and depositional history of Coniacian-Santonian succession in East of Ramhormoz area (Tange-Bulfaris section)
This study is focused on the biostratigraphy, sedimentary environments, facies distribution, and sequence stratigraphy of the Coniacian–Santonian sediments of Tange-Bulfaris section. Five assemblage zones have been recognized by distribution of the foraminifera in the study area. Assemblage zone 1(Chara Ostracods zone) is Coniacian in age and occurs in the lower part of the succession. Assembl...
متن کاملThermal and catalytic degradation study of polyethylene and investigation the catalytic effect of X-Zeolite and Silica-Alumina on degradation kinetic
The thermal degradation of polyethylene (PE) was carried out in the absence and presence ofcatalystes X-Zeolite and Silica-Alumina at different temperatures. The optimum PE/Catalysisratio was 0.25:0.05 g/g, which produced highest degradation value. PE and PE/Catalysis werecharacterized by thermogravimetric analysis. The thermal degradation properties of polymerhave been studied by Infrared spec...
متن کاملMicrobial consortium to degrade plastic pdf
Due to plastics resilience against degradation and its proliferation in. An extremely halotolerant bacterial consortium MPD-M, immobilized.The hypothesis is that if PE-degrading microorganisms do exist in the Nature, then it will be possible to isolate them and use them for degradation of plastic bags. A microbial consortium capable of PE degradation was obtained as a result of.Selection and sc...
متن کامل