In Vitro Comparative Analysis of Fracture Resistance in Inlay Restoration Prepared with CAD-CAM and Different Systems in the Primary Teeth

نویسندگان

  • Huseyin Simsek
  • Sera Derelioglu
چکیده

Objective. The aim of this study was to compare to fracture resistance test of inlay restorations prepared using direct inlay technique (Gradia® Direct Composite) and Indirect Restoration System® (Gradia Indirect Composite) and CAD/CAD system (Vita Enamic® Block). Study Design. 48 noncarious extracted maxillary second primary molars were randomly divided into 4 groups with 12 in each group. All the teeth were prepared based on inlay class II preparations except for the control group. Other groups were restored with Gradia Direct Composite, Gradia Indirect Composite, and Vita Enamic Block, respectively. All restorations were cemented self-adhesive dual cure resin (3M Espe, RelyX™ Unicem Aplicap). A fracture test was performed using a compressive load. Results were analyzed using one-way analysis of variance and Duncan's post hoc multiple comparison tests (α = 0.05). Results. Vita Enamic Block and Gradia Indirect Composite showed significantly higher fracture resistance than Gradia Direct Composite (p < 0.05). There was no significant difference fracture resistance between Vita Enamic Block and Gradia Indirect Composite (p > 0.05). All restorations tested led to a significant reduction in fracture resistance (p < 0.05). Conclusion. In inlay restorations, Indirect Restoration Systems and CAD/CAM systems were applied successfully together with the self-adhesive dual cure resin cements in primary molars.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

بررسی مقاومت به شکست اینله بریج‌های Fiber-Reinforced Composite قدامی بالا و خلفی پایین در شرایط in vitro

Background and Aim: Considering flexural strength of fiber-reinforced composites (FRC) and also the role of conservative cavities in protecting sound tissue of abutments, the aim of this study was to evaluate the fracture resistance of these bridges by handmade samples in vitro.Materials and Methods: In this experimental in vitro study, 44 sound newly extracted teeth were used to make 22 fixed ...

متن کامل

In Vitro Evaluation of Fracture Resistance of Zirconia Restorations Veneered by Two Different Systems: Rapid Layer Technique and Zir/CAD/CAM

Background: This study aimed to assess the fracture resistance of zirconia restorations fabricated with rapid layer (RL group) technique and zirconia computer-aided design/computer-aided manufacturing (zir/CAD/CAM) system (ZC group). Methods:This study evaluated 30 all-ceramic crowns in two groups of 15. After fabricating the metal dies and scanning them ...

متن کامل

In-Vitro evaluation of fracture resistance of weakened roots restored with fiber posts and tooth-colored materials

In-Vitro evaluation of fracture resistance of weakened roots restored with fiber posts and tooth-colored materials Dr. H. Moosavi* - Dr. F. Maleknejad**- Dr. I. Nasiraee*** * Assistant Professor of Operative Dentistry Dept., Faculty of Dentistry, Mashhad University of Medical Sciences. ** Associate Professor of Operative Dentistry Dept., Faculty of Dentistry, Mashhad University of Medical Scien...

متن کامل

Fracture Resistance of Maxillary Primary Anterior Restorations Using Grandio and Grandio Flow Composites with Two Differ-ent Types of Posts: An In Vitro Study

Background and Aim: There have been attempts to restore destroyed primary anterior teeth using a variety of post and core systems, which were able to solve just part of the problems related to this issue. Therefore, the present study aimed to inves-tigate the fracture resistance of restorations supported with a variety of posts and cores in primary anterior teeth. Materials and Methods: The pr...

متن کامل

Influence of different composite materials and cavity preparation designs on the fracture resistance of mesio-occluso-distal inlay restoration.

The aim of the study to evaluate the fracture resistance of a computer-aided design/computer-aided manufacturing (CAD/CAM) and three indirect composite materials for three different mesio-occluso-distal (MOD) inlay cavity designs. A total of 120 mandibular third molar were divided into three groups: (G1) non-proximal box, (G2) 2-mm proximal box, and (G3) 4-mm proximal box. Each cavity design re...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 2016  شماره 

صفحات  -

تاریخ انتشار 2016