Nanoindentation has been used to study the hardness changes produced by scratching of aluminium alloy AA2024, with and without a clad layer of pure aluminium. The hardness was mapped around scratches made with diamond tools of different profiles. One tool produced significant plastic damage with associated hardening at the scratch root, whilst the other produced a ‘cleaner’ cut with no hardening. The different behaviours and are attributed to whether the tool makes the scratch by a ‘cutting’ or a ‘ploughi g’ mechanism. The degree of plastic damage around the scratches has been correlated with peak broadening data obtained using synchrotron X-ray diffraction. There was no change observed in the local hardness around the scratch with fatigue loading.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Friction Stir Welded 2024-T351 Aluminium Alloy

Fatigue failure characteristics of friction stir welds in 13mm gauge 2024-T351 plate have been assessed. Failure occurred from either the weld region (nugget/flow arm) or from the material immediately surrounding the weld. Fatigue failure from the surrounding material was essentially conventional, initiating from large S-phase intermetallic particles and growing in a macroscopic mode I manner. ...

متن کامل

Strengthening Mechanisms in the Aged 2024 and 7075 Aluminium Alloys

Aluminum 2024 and 7075 alloys which are widely used in aerospace and marine applications were chosen to investigate their strengthening mechanisms. Using differential thermal analysis (DIA), metallography and tension tests, the best solutionizing conditions were determined to be 500±5°C and 2 hours for 2024 and 480?±5°C and 1 hour for 7075 alloy. Aging was performed in the range of 100 to 200°C...

متن کامل

TENSILE AND FRACTURE CHARACTERISTICS OF A SIC- PARTICLE-REINFORCED 7075 ALUMINIUM ALLOY

Fracture behavior of a 7075 aluminium alloy reinforced with 15 Vol%. SiC particles was studied after T6 and annealing heat treatments under uniaxial tensile loading at room temperature. The scanning electron microscopy of fractured surfaces and EDS analysis showed:, that fracture mechanism changed from due mainly to fractured particle in T6 condition to interface decohesion in samples in anneal...

متن کامل

Effect of friction stir welding parameters on the microstructure and mechanical properties of dissimilar AA2024-AA6061 joints

In the present study, to resolve the problems in fusion welding methods as well as to increase the strength, FSW method was used to join aluminum alloy sheets 6061 and 2024. Moreover, optimal parameters for joining of these two alloys were also taken into consideration. Various tool rotation speeds of 565, 950 and 1500 rpm were selected. For each tool rotation speed, two traverse speed variable...

متن کامل

EFFECT OF T6 HEAT TREATMENT ON MECHANICAL PROPERTIES OF CERAMIC REINFORCED CASTED ALUMINUM ALLOY

Aluminium base alloy (Al-Cu-Si) was reinforced with silicon carbide (SiC) particles, in various percentage compositions from 0-20 wt%. Silicon carbide particle size of 20µm was selected. The molten slurry of SiC reinforced base aluminium metal was casted through green and dry sand casting methods and solidification process was carried out under ambient conditions. A selected population...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2009