Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses.

نویسندگان

  • A H De Aza
  • J Chevalier
  • G Fantozzi
  • M Schehl
  • R Torrecillas
چکیده

Mono-phase bio-ceramics (alumina and zirconia) are widely used as femoral heads in total hip replacements (THR) as an alternative to metal devices. Unfortunately, the orthopaedic community reports significant in-vivo failures. Material scientists are already familiar with composites like alumina zirconia. Since both are biocompatible, this could prove to be a new approach to implants. This paper deals with a new generation of alumina-zirconia nano-composites having a high resistance to crack propagation, and as a consequence may offer the option to improve lifetime and reliability of ceramic joint prostheses. The reliability of the above mentioned three bio-ceramics (alumina, zirconia and zirconia toughened alumina) for THR components is analysed based on the study of their slow crack-growth behaviour. The influence of the processing conditions on the microstructure development, of the zirconia toughened alumina composites and the effect of these microstructures, on its mechanical properties, are discussed.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Slow-Crack-Growth Behavior of Zirconia-Toughened Alumina Ceramics Processed by Different Methods

A study of slow-crack propagation in zirconia-toughened alumina (ZTA) ceramics is presented. Different ZTA composites, using either unstabilized or yttria-stabilized zirconia, have been tested. The materials were prepared in the range 0–15 vol% ZrO2, using two processing methods: powder mixing and a modified colloidal route. Crack propagation tests have been conducted for crack velocities from ...

متن کامل

Degradation of alumina and zirconia toughened alumina (ZTA) hip prostheses tested under microseparation conditions in a shock device

This paper considers the degradation of alumina and zirconia toughened alumina vs. alumina for hip implants. The materials are as assumed to be load bearing surfaces subjected to shocks in wet conditions. The load is a peak of force; 9 kN was applied over 15 ms at 2 Hz for 800,000 cycles. The volumetric wear and roughness are lower for ZTA than for alumina. The long ZTA ageing did not seem to h...

متن کامل

Fracture Toughness of Advanced Ceramics at Room Temperature

This report presents the results obtained by the five U.S. participating laboratories in the Versailles Advanced Materials and Standards (VAMAS) round-robin for fracture toughness of advanced ceramics. Three test methods were used: indentation fracture, indentation strength, and single-edge pre-cracked beam. Two materials were tested: a gas-pressure sintered silicon nitride and a zirconia tough...

متن کامل

Fibrous Monolithic Ceramics: I , Fabrication, Microstructure, and Indentation Behavior

Monolithic ceramics have been fabricated from coated green fibers to create fibrous microstructures. The fibrous monoliths consist of high aspect ratio polycrystalline regions (cells) of a primary phase separated by thin secondphase regions (cell boundaries) designed to improve fracture resistance. The cells are the remnants of the green fiber which consists of ceramic powder and a polymer bind...

متن کامل

Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations.

The lifetime of a ceramic is dependent on the presence of incidental cracks and their gradual propagation under the conditions of the oral cavity. The objective of this study was to examine the long-term strength of glass-infiltrated alumina- and various zirconia ceramics currently used in CAD/CAM systems to manufacture crown and bridge frameworks. Fracture mechanics were applied to determine c...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Biomaterials

دوره 23 3  شماره 

صفحات  -

تاریخ انتشار 2002