Comparative assessment of marginal accuracy of grade II titanium and Ni–Cr alloy before and after ceramic firing: An in vitro study

نویسندگان

  • Abhijit Patil
  • Kishan Singh
  • Sukant Sahoo
  • Suraj Suvarna
  • Prince Kumar
  • Anupam Singh
چکیده

OBJECTIVE The aims of the study are to assess the marginal accuracy of base metal and titanium alloy casting and to evaluate the effect of repeated ceramic firing on the marginal accuracy of base metal and titanium alloy castings. MATERIALS AND METHODS Twenty metal copings were fabricated with each casting material. Specimens were divided into 4 groups of 10 each representing base metal alloys castings without (Group A) and with metal shoulder margin (Group B), titanium castings without (Group C) and with metal shoulder margin (Group D). The measurement of fit of the metal copings was carried out before the ceramic firing at four different points and the same was followed after porcelain build-up. RESULTS Significant difference was found when Ni-Cr alloy samples were compared with Grade II titanium samples both before and after ceramic firings. The titanium castings with metal shoulder margin showed highest microgap among all the materials tested. CONCLUSIONS Based on the results that were found and within the limitations of the study design, it can be concluded that there is marginal discrepancy in the copings made from Ni-Cr and Grade II titanium. This marginal discrepancy increased after ceramic firing cycles for both Ni-Cr and Grade II titanium. The comparative statistical analysis for copings with metal-collar showed maximum discrepancy for Group D. The comparative statistical analysis for copings without metal-collar showed maximum discrepancy for Group C.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

بررسی تطابق لبه‌ای بین دو نوع رستوریشن زیرکونیایی Cercon و Zirkonzahn قبل و بعد از پرسلن‌گذاری

Background and Aims: The marginal integrity of fixed restorations always is a major matter of concern for dental clinicians. Any cause of distortion, including veneering processes, in the marginal integrity is supposed to be detrimental for long-term success of fixed dental prostheses. The aim of this in vitro study was to compare the marginal adaptation of two different full ceramic restoratio...

متن کامل

Marginal fit at cylinder-abutment interface before and after overcasting procedure.

The aim of this study was to measure marginal fit at cylinder-abutment interface, before and after overcasting procedure. A hexagonal implant was fixed to a stainless steel base and a Estheticone-like abutment used during all the experiment. Before casting procedure, gold (Group I) and Ni-Cr-Be (Group II) premachined cylinders were tightened to the abutment with gold and titanium screws (in bot...

متن کامل

بررسی و مقایسه زیست‌سازگاری آلیاژ مینالوکس و آلیاژ مشابه خارجی (In-vitro)

Statement of Problem: One of newly presented base metal alloys (Minalux) is produced according to VeraBond2 alloy (Ni- Cr base) composition. Several studies showed that, cytotoxicity of base metal alloys can be occurred due to corrosion and element release. Purpose: This study evaluated the biocompatibility of these two base metal alloys in three steps: as cast, after polishing and after porcel...

متن کامل

Comparative Evaluation of Microgap at the Interface of Titanium and Zirconium Abutments Following Oblique Cyclic Loading: An in vitro Study

Abstract   Background and Aim : Microgap in the implant-abutment interface is one of the main challenges in the treatment of two-piece implants. This study aimed to investigate the effect of two types of abutments (zirconia and titanium) on microgap at implant-abutment interface area under oblique cyclic loading in vitro. Methods and Materials In this in vitro study, 12 implant-abutment assemb...

متن کامل

Bond strength of three dental porcelains to Ni-Cr and Co-Cr-Ti alloys.

Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cy...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 7  شماره 

صفحات  -