Glyceryl Methacrylate Asa Dentin Primer

نویسندگان

  • Kazuo ITOH
  • Sadao WAKUMOTO
  • Tohru HAYAKAWA
چکیده

The eMcacy of pretreatment on the dentin surface with an aqueous solution of glycery1 methacrylate {GM) was examined by measuring the wall-to-wall polymerization centraction of a light activated composite in a cylindrical dentin cavity, and by measuring the tensile bondi strength to a flat dentin surface. All of the tested dentin surfaces were cleaned with neutralized O.5M EDTA and treated with experimental primers, followed by a marketed dentin bonding agent and composite. The contraction gap forination of the composite was completely prevented by the application of the GM solution at concentrations of 25 and 35% in water. In contrast, half of the specimens treated with 35% HEMA and 35% HEMA containing 5% glutaraldehyde showed gap forrnation, Furthermore, a considerably high tensile bond strength of more than 18MPa was observecl in the above described entin bonding system.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Possibility of allergic reaction to dentin primer--application on the skin of guinea pigs.

We studied the allergic reaction of guinea pigs to glyceryl methacrylate (GM), hydroxyethyl methacrylate (HEMA) and meso-erythritol methacrylate (EM), which are used as dentin primers. On the 18th day of the application test, when macroscopic investigation revealed an inflammatory reaction, the methacrylic acid-treated group showed marked eschar formation in comparison with the control group. I...

متن کامل

Efficacy of glyceryl methacrylate as a dentin primer.

The efficacy of pretreatment on the dentin surface with an aqueous solution of glyceryl methacrylate (GM) was examined by measuring the wall-to-wall polymerization contraction of a light activated composite in a cylindrical dentin cavity, and by measuring the tensile bond strength to a flat dentin surface. All of the tested dentin surfaces were cleaned with neutralized 0.5 M EDTA and treated wi...

متن کامل

The efficacy of dentine adhesive to sclerotic dentine.

OBJECTIVE To evaluate the effect of a dentine bonding system to sclerotic dentine in comparison with normal dentine. METHODS The efficacy of the dentine bonding system to sclerotic dentine was examined by measuring wall-to-wall polymerization contraction gap width. The dentine cavity wall was pretreated with an experimental dentine bonding system with and without a dentine primer. The dentine...

متن کامل

Effect of 4-acryloxyethyltrimellitic acid in a self-etching primer on bonding to ground dentin.

To develop a self-etching primer for ground dentin, 4-acryloxyethyltrimellitic acid (4-AET) was newly synthesized, and the effect of concentrations varying from 0 (control) to 56.5 wt% 4-AET in the water/ HEMA primer on bonding to the dentin was investigated. Bond strength to the dentin was significantly affected by the inclusion of 4-AET in the primer which also contained N,N-di(hydroxyethyl)-...

متن کامل

Curing Units and Dentin Thicknesses

of two restorative composite resins (Filtek P90 silorane-based composite and Heliomolar methacrylate-based composite) with either a quartz-tungsten-halogen (QTH) or lightemitting diodes (LED) light-curing unit (LCU) and using dentin thicknesses (0.5 and 1.0 mm). Standardized cavities (2x2x2 mm) were prepared in 80 bovine incisors, which were randomly assigned to 8 groups according to the photoa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2017