Based on the engineering background of water dissolving mining for hydrocarbon storage in multi-laminated salt stratum, the mixed mode fracture toughness and fracture trajectory of gypsum interlayers soaked in half-saturated brine at various temperatures (20°C, 50°C and 80°C) were studied by using CSNBD (centrally straight-notched Brazilian disc) specimens with required inclination angles (0°, 7°, 15°, 22°, 30°, 45°, 60°, 75°, 90°) and SEM (scanning electron microscopy). The results showed: (i) The fracture load of gypsum specimens first decreased then increased with increasing inclination angle, due to the effect of friction coefficient. When soaked in brine, the fracture toughness of gypsum specimens gradually decreased with increasing brine temperature. (ii) When soaked in brine, the crystal boundaries of gypsum separated and became clearer, and the boundaries became more open between the crystals with increasing brine temperature. Besides, tensile micro-cracks appeared on the gypsum crystals when soaked in 50°C brine, and the intensity of tensile cracks became more severe when soaking in 80°C brine. (iii) The experimental fracture envelopes derived from the conventional fracture criteria and lay outside these conventional criteria. The experimental fracture envelopes were dependent on the brine temperature and gradually expanded outward as brine temperature increases. (iv) The size of FPZ (fracture process zone) was greatly dependent on the damage degree of materials and gradually increased with increase of brine temperature. The study has important implication for the control of shape and size of salt cavern.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mixed Mode Fracture in Reinforced Concrete with Low Volume Fraction of Steel Fibers

An investigation into the mixed mode fracture of steel fiber reinforced concrete (SFRC)beams with one percent volume fraction of steel fiber is presented. A series of notched beams withdifferent notch depths and locations are tested under three-point bending. The test results for apparentfracture toughness, crack trajectories, and fracture energy are presented. The crack paths for SFRCand plain...

متن کامل

Effects of temperature and confining pressure on mode II fracture toughness of rocks (Case study: Lushan Sandstone)

The fracture mechanics examines the development and expansion of cracks in solids and how they affect the deformation of materials. The stress intensity factors at the tip of the crack and the critical stress intensity factors or fracture toughness of materials are considered in the relevant criteria. There are three main modes of applying forces to a crack including the tensile mode, shear mod...

متن کامل

Mixed-mode I/II Interlaminar Fracture of CF/PEI Composite Material

Failures in composite materials occur mainly due to interlaminar fracture, also called delamination, between laminates. This indicates that characterizing interlaminar fracture toughness is the most effective factor in the fracture of composite materials. This study reports investigation on mixed-mode interlaminar fracture behaviour in woven carbon fibre/polyetherimide (CF/PEI) thermoplastic co...

متن کامل

Effects of number of freeze-thaw cycles and freezing temperature on mode I and mode II fracture toughness of cement mortar

Natural and artificial materials including rocks and cement-based materials such as concrete and cement mortar are affected both physically and chemically by various natural factors known as weathering factors. The freeze-thaw process, as a weathering factor, considerably affects the properties of rocks and concrete. Therefore, the effect of the freeze-thaw process on the physical and mechanica...

متن کامل

Study of Variation of the J-integral and the Fracture Toughness in Blunt V-notches under Mode I Loading

Fracture assessment of U- and V-notches is important in mechanical engineering. One can use the J-integral as fracture parameter in order to predict the critical fracture load in notches. The critical value of the J-integral in cracks is a function of the material properties. In notches, however, the material properties as well as the notch dimensions affect this critical value (named fracture ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 5  شماره 

صفحات  -

تاریخ انتشار 2018