Dynamic Shear Behaviour of Unweldable Aluminum-Scandium (Al-Sc) Alloy
نویسندگان
چکیده
This study uses a torsional split-Hopkinson bar to investigate the shear response and fracture characteristics of unweldable Al-Sc alloy during mechanical testing at shear strain rates of 800 s , 1500 s , 2200 s 1 and 2800 s 1 and temperatures of 150 C, 25 C and 300 C. The experimental results show that both the shear strain rate and the temperature have a significant effect on the shear properties of the Al-Sc alloy. At a constant temperature, the shear stress, fracture shear strain, work hardening rate, yielding shear strength, work hardening coefficient, strain rate sensitivity and temperature sensitivity all increase with increasing strain rate. However, inverse tendencies are observed with increasing temperature at a constant strain rate. It is found that the Kobayashi and Dodd constitutive equation provides accurate predictions of the high strain rate shear plastic behaviour of unweldable Al-Sc alloy. SEM fractographic observations reveal that the fracture surfaces are characterized by a dimple-like structure. The density of the dimples increases with increasing strain rate at a constant temperature or with increasing temperature at a constant strain rate. SEM observations indicate that specimen fracture initiates at the interface of the matrix and the Al3Sc precipitates. Finally, twisted shear bands are observed on the equatorial plane of the gauge length section of the deformed specimens. The microhardness of these shear bands increases with increasing strain rate, but decreases with increasing temperature. [doi:10.2320/matertrans.48.500]
منابع مشابه
THERMAL ANALYSIS AND KINETICS OF THE PRECIPITATION IN WROUGHT Al-Mg, Al-Mg-ScAND Al-Mg-Sc-Me (Me=Zr, Ti) ALLOYS
Precipitation behaviour of wrought Al-6Mg alloys with ternary scandium and quaternary zirconium and titanium has been studied. Hardness measurements and resistivity studies are employed to assess the precipitation behaviour of scandium doped Al-6Mg alloy without or with quaternary additions of zirconium and titanium. Further, the kinetics of precipitations are studied by differential scanning c...
متن کاملFRACTIONAL RECRYSTALLIZATION KINETICS IN DIRECTLY COLD ROLLED Al-Mg, Al-Mg-Sc AND Al-Mg-Sc-Zr ALLOY
The evaluation of texture as a function of recrystallization has been characterized for directly cold rolled Al-6Mg, Al-6Mg-0.4Sc and Al-6Mg-0.4Sc-0.2Zr alloys. Samples were annealed isothermally at 400 °C for 1 to 240 minutes to allow recrystallization. Recrystallization kinetics of the alloys is analyzed from the micro-hardness variation. Isothermally annealed samples of aluminum alloys were ...
متن کاملPrecipitation Hardening Behavior of Directly Cold Rolled Al-6Mg Alloy Containing Ternary Sc and Quaternary Zi/Ti
Ageing of 75% cold rolled Al-6Mg alloy with ternary 0.4 wt% scandium and quaternary zirconium and titanium has been carried out. Alloy samples are naturally, isochronally and isothermally aged for different time and temperatures. Hardness values of the differently processed alloys have been measured to understand the ageing behavior of Al-6Mg alloy with scandium and quaternary zirconium and tit...
متن کاملScandium-Enriched Nanoprecipitates in Aluminum Providing Enhanced Coarsening and Creep Resistance
The development of high temperature aluminum alloys able to operate up to 400 oC is crucial to replace steel and titanium and decrease the mass of vehicles in the automotive and aerospace industries. This review relates the past two decades of aluminum alloy engineering done at Northwestern University focusing on developing coherent L12 Al3M nanoprecipitates strengthened aluminum alloys that ar...
متن کاملExperimental Analysis of Microstructure and Mechanical Behaviour in Fine Grained Al-Zn-Mg Alloy
The high strength Al-Zn-Mg alloy is widely used for structure components in critical aerospace applications. Small additions of scandium (Sc) often refine cast microstructure and mechanical properties by forming metastable Al3Sc dispersoids. The main role of the Al3Sc dispersoid is to prevent recrystallization during hot deformation and solution treatment. A new technique to apply for surface m...
متن کامل