Film Thickness and Flow Properties of Resin-Based Cements at Different Temperatures
نویسنده
چکیده
STATEMENT OF PROBLEM For a luting agent to allow complete seating of prosthetic restorations, it must obtain an appropriate flow rate maintaining a minimum film thickness. The performance of recently introduced luting agents in this regard has not been evaluated. PURPOSE To measure and compare the film thickness and flow properties of seven resin-containing luting cements at different temperatures (37°C, 25°C and10°C). MATERIAL AND METHODS Specimens were prepared from five resin luting cements; seT (SDI), Panavia F (Kuraray), Varioloink II (Ivoclar), Maxcem (Kerr), Nexus2 (Kerr) and two resin-modified glass-ionomer luting cements (RM-GICs); GC Fuji Plus (GC Corporation), and RelyX Luting 2 (3 M/ESPE). The film thickness and flow rate of each cement (n=15) was determined using the test described in ISO at three different temperatures. RESULTS There was a linear correlation between film thickness and flow rate for most of the materials. Cooling increased fluidity of almost all materials while the effect of temperature on film thickness was material dependent. At 37°C, all products revealed a film thickness of less than 25µm except for GC Fuji Plus. At 25°C, all cements produced a film thickness of less than 27 µm except for seT. At 10°C, apart from seT and Rely X Luting 2, the remaining cements showed a film thickness smaller than 20 µm. CONCLUSION Cooling increased fluidity of almost all materials, however. the film thickness did not exceed 35 µm in either condition, in spite of the lowest film thickness being demonstrated at the lowest temperature.
منابع مشابه
بررسی خواص فیزیکی سمان موقت ایرانی Tem Band و سمان موقت خارجی Temp Bond و مقایسه آنها با ISO 3107
Background and Aim: Iranian temporary cement, Tem Band, has been manufactured by Golchai company, and introduced to market as a suitable material but its properties have not been tested yet. The aim of this study was to investigate the setting time, film thickness, compressive strength, disintegration and arsenic content of Tem Band and Temp bond temporary cements and compare them to ISO 3107. ...
متن کاملFilm thickness of resin cements used with adhesive systems.
The final film thickness of a resin adhesive and a resin cement could be affected by previous polymerization of the adhesive systems on dentin surfaces. The aim of this work was to evaluate changes in the film thickness of dual resin based cements with their adhesives as a function of polymerization of the latter on dentin surfaces. The materials used were: RelyX ARC (R) + Single Bond (SB) and ...
متن کاملEvaluating the effect of ceramic veneer thickness on degree of conversion in three luting resin cements
compare the effect of different ceramic thicknesses on degree of conversion (DC) of 3 light-cured resin cements. Methods: In this experimental in-vitro study, the degree of conversion of three light-cured resin cements, Variolink Veneer (Ivoclar, Liechtenstein), RelyX Veneer (3M ESPE, USA) and Choice2 (Bisco, USA) were evaluated beneath feldespatic ceramic discs (Vita VMK Master) with a same sh...
متن کاملIn vitro evaluation of the film thickness of self-etching resin cements.
The aim of this study was to evaluate the film thickness of selfetching resin cement. The following materials were used: Group1, Relyx U100 (3M /ESPE); Group 2, BisCem (Bisco); Group 3, Max Cem (Kerr); Group 4, Set (SDI) and Group 5, Relyx ARC (3M/ESPE) as control. Two 5.4 x 76.2 x 1 mm glass slides were marked in the center to identify the area where the material would be placed. A volume of 0...
متن کاملFracture Resistance of Lithium Disilicate Ceramics Bonded to Enamel or Dentin Using Different Resin Cement Types and Film Thicknesses.
PURPOSE To investigate the influence of cement film thickness, cement type, and substrate (enamel or dentin) on ceramic fracture resistance. MATERIALS AND METHODS One hundred extracted human third molars were polished to obtain 50 enamel and 50 dentin specimens. The specimens were cemented to 1-mm-thick lithium disilicate ceramic plates with different cement film thicknesses (100 and 300 μm) ...
متن کامل