Coatings control corrosion by providing a barrier against oxygen and water. Although coatings are extremely effective, all organic coatings are semi-permeable to O2 and water. The water permeability coefficient of fusion bonded epoxies, one of the best coating systems, is approximately 10 gms/mil/24 hours, but minimum concentration of oxygen and water that can start the corrosion process is 10 M. In this paper, Nernst equation is used to calculate these concentrations. Cathodic Protection, CP, on the other hand controls corrosion by providing excess electrons to the pipe surface. This system is based on the electrical circuit, where the negative terminal of electrical source is connected to the pipe and the positive terminal to the anode that is placed in the soil. Both systems have limitations in providing the absolute protection single handedly. A combination of CP and coating is the best solution for this complex problem. In the CP-Coating System, coating undertakes the major role to provide the needed protection and CP assumes the secondary role. However, in all cases where the coating fails to provide protection, CP becomes critically important and should provide the necessary protection. Therefore, the limitations of each system should be evaluated and their properties must be adjusted so that they will work in union. In this paper, the properties of coatings that are critical in making the coating a part of the CP-Coating Combination System are discussed. Adhesive Strength and Cohesive Strength are two important and two distinctively different properties. Adhesive Strength is a total sum of several components. Mechanical adhesion, polar-polar adhesion and chemical adhesion are three major components of Adhesive Strength of the coating. The role of these (adhesion and cohesion) properties in providing long-term protection are explained. Along with the chemistry of the coating, the application parameters have a major role in the final Adhesive Strength of the coating. In this paper, the important parameters that control the adhesive strength and how they depend on some of the application parameters are also explained.
منابع مشابه
An Electrochemical Measurement for Evaluating the Cathodic Disbondment of Buried Pipeline Coatings under Cathodic Protection
Steel pipelines are susceptible to corrosion by the action of corrosive substance in the environment and one of the most common failure modes in buried pipeline coatingis cathodic disbondment. Consequently, Electrochemical Impedance Spectroscopy (EIS) was used to assess the effect of three important parameters, the thickness of coating, the artificial defect ...
متن کاملEnergy Management Strategy of Stand-alone Photovoltaic System in Cathodic Protection Pipeline
In this paper, the stand-alone photovoltaic system for cathodic protection of underground pipelines is presented. The proposed system offers continuous and automatic adjustment of the applied voltage so that the buried pipelines receive the exact current. A modified perturb and observe (P&O) algorithm for maximum power point tracking (MPPT) is used to improve dynamic and steady state performa...
متن کاملA Review on Studies and Research on Corrosion and Its Prevention
Corrosion is one of the major reasons for wear and tear of equipments. It is also responsible for reducing the life of equipments. Many accidents occur because of failure of pipelines due to corrosion. There are many methods to minimize corrosion. Cathodic protection, use of inhibitors, use of anticorrosive coatings is few methods used for this purpose. The presence of moisture in the atmospher...
متن کاملEvaluation of Heat Treatments and Their Effects on the Corrosion Behavior of TiAlON Coatings Prepared by Cathodic Arc Evaporation on D3 Tool Steel
A series of TiAlON coatings were synthesized in a gaseous mixture of argon, nitrogen and oxygen by cathodic arc evaporation method using a Ti–Al mosaic target. Oxidation of coatings was carried out by heating the coated samples at the temperatures of 500, 600, 700, and 800°C for 1 h in air atmosphere. It was found that heat treatment changed the microstructure and composition of the coating. Th...