Post-synthesis Annealing Effects on SrGa2Se4:Eu Phosphors with Peak Emission Wavelength in the Green Gap
نویسندگان
چکیده
A high-quality white light source requires high luminous efficacy (lumens per input watt). Theoretically, in the “greenyellow” spectral region (with a peak wavelength at around 555 nm), the luminous efficiency (lumens per radiant watt) reaches a maximum based on the luminous efficiency function, V(λ), and can potentially generate high luminous efficacy. Unfortunately, the light-emitting diode (LED) suffers from low external quantum efficiency in the “greenyellow” region, thereby lowering the luminous efficacy value. Researchers have sought solutions such as nonpolar or semipolar InGaN/GaN LEDs. An alternative to generating green light is to use phosphor down-conversion by exciting a green emission phosphor with a near-UV or blue LED of higher external quantum efficiency. In this study, a SrGa2Se4:Eu phosphor with peak emission wavelength at 555 nm was initially synthesized and followed by a systematic study of the post-synthesis annealing. The purpose of this study was to investigate how post-synthesis annealing conditions, including annealing temperature, annealing duration, and annealing ambient atmosphere, can affect phosphor performance. The phosphor performance was characterized in terms of external quantum efficiency and emission properties. How the external quantum efficiency of the phosphor can be further improved is also discussed.
منابع مشابه
The Effect of Heat Treatment on the Emission Color of P-Doped Ca2SiO4 Phosphor
In a series of (Ca2-x/2-yEuy□x/2)(Si1-xPx)O₄ (x = 0.06, 0.02 ≤ y ≤0.5), various color-emitting phosphors were successfully synthesized by a solid-state reaction. These phosphors were characterized by photoluminescence (PL) spectroscopy, X-ray powder diffractometry, transmission electron microscopy, and X-ray absorption fine structure spectroscopy. We evaluated the effect of heat treatment on PL...
متن کاملPechini synthesis of lanthanide (Eu3+/Tb3+or Dy3+) ions activated BaGd2O4 nanostructured phosphors: an approach for tunable emissions.
Trivalent lanthanide (Eu(3+), Tb(3+) and Dy(3+)) ions activated tunable color emitting BaGd2O4 (BG) phosphors were synthesized by a facile Pechini-type sol-gel process. The X-ray diffraction pattern confirmed the orthorhombic phase after annealing at 1300 °C for 5 h. Morphological studies were performed based on the analysis of transmission electron microscopy images, which showed needle type n...
متن کاملSynthesis and Characterization of Nb2O5:La,Eu Phosphors Obtained by the Non‐Hydrolytic Sol‐Gel Process
The phosphor-converted light-emitting diode technique is an important solid-state illumination strategy. Sulfide-based materials are the most often employed red phosphors, but they are chemically unstable and present lower efficiency in comparison to the blue and green phosphors. Therefore, it is important to find a new red phosphor source that can emit intense red light while absorbing light i...
متن کاملSynthesis of Green-Emitting (La,Gd)OBr:Tb3+ Phosphors
Green-emitting phosphors based on lanthanum-gadolinium oxybromide were synthesized in a single phase form by the conventional solid state reaction method, and photoluminescence properties of them were characterized. The excitation peak wavelength of (La1-xGdx)OBr:Tb 3+ shifted to the shorter wavelength side with the increase in the crystal field around the Tb 3+ ions by doping Gd 3+ ions into t...
متن کاملVersatile properties of CaGd₂ZnO₅:Eu³⁺ nanophosphor: its compatibility for lighting and optical display applications.
Red color-emitting CaGd2ZnO5:Eu(3+) (CGZO:Eu(3+)) nanophosphors were synthesized by a facile sol-gel process. The structural and luminescent properties of these phosphors were investigated as a function of annealing temperature and Eu(3+) ion concentration. The orthorhombic phase was confirmed at different annealing temperatures, showing an irregular morphology within the nanoscale range. Photo...
متن کامل