Effect of surface condition of dental zirconia ceramic (Denzir) on bonding.
نویسندگان
چکیده
Yttria partially stabilized zirconia (YPSZ) ceramics are suitable for dental and medical use because of their high fracture toughness and chemical durability. The purpose of this study was to examine the bonding behavior of a dental YPSZ ceramic, Denzir. After being subjected to various surface treatments, Denzir specimens were bonded to each other using an adhesive resin composite, glass ionomer, or zinc phosphate cement. Bonding strength was then determined by the shearing test. No significant differences (p>0.05) were observed between SiC- and Al2O3-blasted specimens. In all surface treatments, the shear bond strength significantly (p<0.05) increased in the order of adhesive resin composite cement > glass ionomer cement > zinc phosphate cement. Moreover, silanization with methacryloxy propyl trimethoxysilane slightly increased the bonding strength of the adhesive resin composite cement.
منابع مشابه
Effect of Laser Irradiation on Bond Strength of Zirconia Ceramic to Self-Adhesive Resin Cement
Background and Aim: Bonding of zirconia to resin cement is challenging, and the zirconia surface requires surface treatment to yield an acceptable bond strength. This study aimed to evaluate the effect of different surface treatments on the bond strength of zirconia to a resin cement. Materials and Methods: In this in-vitro experimental study, 60 zirconia discs measuring 12 mm in diameter an...
متن کاملEffect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites.
Aim of the investigation was to assess the effect of different surface treatments on the bond strength of veneering ceramics to zirconia. In a shear test, the influences of polishing, sandblasting, and silica-coating of the zirconia surface on bonding were assessed with five different veneering ceramics. In addition the effect of liner application was examined. With one veneering ceramic, the i...
متن کاملEffect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown
This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...
متن کاملEffect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics.
This study was conducted to enhance the tensile bond strengths of resin cements to zirconia ceramics. Fifty-six zirconia ceramic specimens (Cercon Base) and twenty-eight silica-based ceramic specimens (GN-1, GN-1 Ceramic Block) were air-abraded using alumina. Thereafter, the zirconia ceramic specimens were divided into two subgroups of 28 each according to the surface pretreatment; no pretreatm...
متن کاملEvaluation of zirconia bonding to veneering porcelain
Zirconium dioxide as core ceramic material for dental crowns and bridges, possess high strength, chemical stability and superior aesthetics after veneering. Veneering ceramic is considered to be the weakest part of all-ceramic restorations. The adhesion between the core and veneering porcelain is based on the manner in which the connection occurs in metal-ceramic structures. Standard procedures...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Dental materials journal
دوره 25 3 شماره
صفحات -
تاریخ انتشار 2006