Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their volume is restricted by anatomic realities what require good yield and fatigue strengths of metal [1].

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue and corrosion fatigue properties of Ti-6Al-4V implant grade titanium alloy in Ringer solution

Nowadays modification of metallic biomaterials which are used as implants for bone and hard tissues replacement is considered as an important subject. In the current study, corrosion fatigue properties of Ti-6Al-4V alloy investigated via Rotating-Bending standard test method and then, the results compared with the fatigue properties of the specimens tested in the same conditions. Scanning elect...

متن کامل

EFFECTS OF TENSILE STRENGTH ON FATIGUE BEHAVIOR AND NOTCH SENSITIVITY OF TI-6AL-4V

In this research, rotating bending fatigue test at minimum to maximum stress ratio of R=-1 was used for investigating the fatigue behavior of Ti-6Al-4V alloy. Both smooth and notched specimens, with elastic concentration factor, kt, of approximately 3.6 and 4.1 were used for this purpose.In addition, the effect of variation in ultimate tensile strength, UTS, on the fatigue behavior of this allo...

متن کامل

A survey of surface treatments to improve the fretting fatigue resistance of Ti-6Al-4V

The effects of surface modification treatments such as shot peening, ion implantation (carbon and nitrogen), surface lubrication (soft coating), laser gas nitriding and various combinations thereof, on the fretting fatigue resistance of Ti-6Al-4V have been investigated. The best of these surface treatments appears to be shot peening. While ion implantation improves the base metal fretting fatig...

متن کامل

Strain-based fatigue data for Ti–6Al–4V ELI under fully-reversed and mean strain loads

This article presents the experimental data supporting the study to obtain the mean strain/stress effects on the fatigue behavior of Ti-6Al-4V ELI. A series of strain-controlled fatigue experiments on Ti-6Al-4V ELI were performed at four strain ratios (-1, -0.5, 0, and 0.5). Two types of data are included for each specimen. These are the hysteresis stress-strain responses for the cycle in a log...

متن کامل

Durability of Fe-Co Thin Films on Ti-6Al-4V

The durability of Fe-Co thin films bonded on Ti-6Al-4V was studied as a function of layer thickness at ambient temperature. Interface toughness of the thin films was characterized by indentation and analyzed using an interface fracture model. The critical stresses for interface debonding and the fatigue life response of Ti-6Al-4V with and without Fe-Co thin films were evaluated by three-point b...

متن کامل

An Experimental Investigation of Fretting Fatigue in Ti-6Al-4V: the Role of Contact Conditions and Microstructure

A systematic investigation of the fretting fatigue behavior of the titanium alloy Ti-6Al-4V in both the mill-annealed (MA) and the solution-treated and overaged (STOA) conditions was carried out. A sphere-on-flat fretting fatigue device was used that facilitated real-time control and monitoring of all the relevant parameters such as the contact geometry, contact (normal and tangential) loads, a...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2012