Comments on "arsenic release provided by MTA and Portland cement" by Duarte MA, et al.

نویسنده

  • Carolyn M Primus
چکیده

The authors presented their data from atomic absorption tests, stating that the cements released less than 0.0007 ppm of arsenic after a week of soaking in weakly acidic solution. That is, the cements released 0.7 ppb from their worst sample. My first comment is on the atomic absorption technique for arsenic. According to the EPA method 7062 for detection of arsenic by atomic absorption using sodium borohydride reduction, the typical detection limit is 1 ␮g/L, which is equal to 1 ppb. These authors are reporting amounts below the normal detection limit for the same method used by the EPA. How did they achieve such results? Second, on page 649, the LD 50 is listed two times for sodium arsenate as 600 mg/kg and also as 10-50 mg/kg. Which is correct? Should one of these have been sodium arsenite? Also, the authors state that they quantified trivalent arsenic, but was any pentavalent arsenic (arsenate) neglected in their analysis? Or did their analysis technique convert all pentavalent to trivalent arsenic? This should have been clarified for the reader. Third, the authors did not report the total arsenic content of the cement they tested. In a report from the Forschungszentrum Karlsruhe GmbH, the average arsenic content of 417 Portland cements was 6.8 ppm. Another study cited in this report found an average of 33 ppm of arsenic. Fourth, the authors did not validate their choice of a solution with a pH equal to 5, nor did they mention any of the dental standards that have solubility requirements to measure As. For instance, ISO 9917, entitled Dental Water-based Cements, has a requirement for lead and arsenic that is appropriate for the Portland cement and ProRoot MTA materials. In ISO 9917, the leachable lead and arsenic must be less than 100 ppm and 2 ppm, respectively. The leaching method is to use hardened, but crushed, cement in a 20% HCl solution for 16 hours. Such a solution has a pH less than 1, considerably more acidic than the authors used. Thirty-six mole percent hydrochloric acid is specified for solubility testing for arsenic in ADA 30 for zinc oxide-eugenol cement. The weakly acidic solution used by the authors did not equal the acidity of vinegar (pH of about 3). Four percent acetic acid, similar to vinegar, is the standard used in testing the solubility of dental porcelain (ISO 9693), not cements. Fifth, Portland cement for construction …

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Arsenic release provided by MTA and Portland cement.

OBJECTIVE The aim of the present study was to determine the release of arsenic from 2 gray Portland cements, a white Portland cement, and 2 MTAs (ProRoot and MTA-Angelus). STUDY DESIGN The materials were manipulated and placed in plastic tubes, and the tubes were immersed in glass flasks containing water with grade reagent, pH 5.0. After 3 and 168 h, the water in which the material had been i...

متن کامل

Presence of arsenic in different types of MTA and white and gray Portland cement.

OBJECTIVE The presence of arsenic in various types of mineral trioxide aggregate (MTA) and Portland cements were evaluated to verify if they comply with the ISO-recommended limit for water-based cements of 2 mg arsenic/kg material. STUDY DESIGN An amount of 5 mL of hydrochloric acid was added to 2 g each of MTA and Portland cement to be analyzed. After 15 minutes, the material was filtered an...

متن کامل

Analysis of heavy metal contents in gray and white MTA and 2 kinds of Portland cement: a preliminary study.

OBJECTIVE The levels of 10 heavy metals (arsenic, bismuth, cadmium, chromium, copper, iron, lead, manganese, nickel, and zinc) in gray Portland cement (GPC), white Portland cement (WPC), gray MTA (GMTA), and white MTA (WMTA) were analyzed by inductively coupled plasma-atomic emission spectrometry (ICP-AES). STUDY DESIGN One gram of each material was digested with 80 degrees C "aqua-regia" (7 ...

متن کامل

Evaluation of physico-chemical properties of Portland cements and MTA.

The purpose of this study was to evaluate the hydrogenionic potential and electrical conductivity of Portland cements and MTA, as well as the amount of arsenic and calcium released from these materials. In Teflon molds, samples of each material were agitated and added to plastic flasks containing distilled water for 3, 24, 72 and 168 h. The results were analyzed with a Kruskal-Wallis non-parame...

متن کامل

Arsenic content in Portland cement: a literature review.

Portland cement (PC) is a hydraulic binding material widely used in the building industry. The main interest in its use in dentistry is focused on a possible alternative to mineral trioxide aggregate (MTA) because PC is less expensive and is widely available. In dentistry, PC has been used in dental procedures such as pulpotomy, pulp capping, repair of root perforation and root-end filling. The...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Oral surgery, oral medicine, oral pathology, oral radiology, and endodontics

دوره 101 4  شماره 

صفحات  -

تاریخ انتشار 2006