Characterising the fracture toughness of polymers at moderately high rates of loading with the use of instrumented tensile impact testing
نویسندگان
چکیده
The more common use of instrumentation in impact testing opened up the possibility to apply fracture mechanics testing methods to polymers at moderately high impact rates. Tensile impact testing offers some advantages over the more common three-point bending and compact tension geometries. Most importantly the dynamic effects encountered at (moderately) high impact rates are less significant due to inherent damping within the specimens. Consequently, the fracture toughness can be determined directly from the force signal without having to employ more sophisticated instrumentation or more elaborate analysis. Despite some unresolved issues the first results on fracture mechanics based tensile impact testing are promising: the toughness values found are comparable to those found using other loading geometries and show less scatter.
منابع مشابه
Strain-rate-dependent mechanical properties of the equine hoof wall.
The mechanical properties of fully hydrated equine hoof wall were examined at various loading rates in compact tension (CT) fracture, tensile and three-point bending dynamic tests to determine possible effects of hoof wall viscoelasticity on fracture toughness and tensile parameters. Four cross-head rates were used in CT tests: 1.7 x 10(-5), 1.7 x 10 (-3), 1.7 x 10(-2) and 2.5ms-1; four strain ...
متن کاملStudy of Variation of the J-integral and the Fracture Toughness in Blunt V-notches under Mode I Loading
Fracture assessment of U- and V-notches is important in mechanical engineering. One can use the J-integral as fracture parameter in order to predict the critical fracture load in notches. The critical value of the J-integral in cracks is a function of the material properties. In notches, however, the material properties as well as the notch dimensions affect this critical value (named fracture ...
متن کاملThe Effect of Microstructure on Estimation of the Fracture Toughness (KIC) Rotor Steel Using Charpy Absorbed Energy (CVN)
The proportional relationships between the Charpy absorbed energy (CVN) and the KIC values have been established for a wide variety of steels. Several formulae have been proposed that predict KIC from CVN. The purpose of this study is to investigate, by means of compact testing fracture toughness specimens, the effective role of microstructure for estimation of the fractur...
متن کاملDynamic and Quasi-Static Tensile Properties of Structural S400 Steel
The study of mechanical behavior of the structural steel S400 under quasi- static and dynamic loading has been the subject of this investigation. In oder to obtain different stress - triaxiality conditions the specimens were notched with 1, 1.5, 2 and 3.5 mm notch radius. The results of fractography show as the velocity of tension increases, ductility reduces and a ductile-brittle transition oc...
متن کاملTENSILE AND FRACTURE CHARACTERISTICS OF A SIC- PARTICLE-REINFORCED 7075 ALUMINIUM ALLOY
Fracture behavior of a 7075 aluminium alloy reinforced with 15 Vol%. SiC particles was studied after T6 and annealing heat treatments under uniaxial tensile loading at room temperature. The scanning electron microscopy of fractured surfaces and EDS analysis showed:, that fracture mechanism changed from due mainly to fractured particle in T6 condition to interface decohesion in samples in anneal...
متن کامل