Load Deflection Characteristics of Nickel Titanium Initial Archwires.

نویسندگان

  • Hossein Aghili
  • Sogra Yasssaei
  • Mahmoud Nilli Ahmadabadi
  • Neda Joshan
چکیده

OBJECTIVES The aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. MATERIALS AND METHODS This study tested three wire designs namely copper nickel titanium (CNT), nickel titanium (NiTi), and multi-strand NiTi (MSNT) archwires engaged in passive self-ligating (PSL) brackets, active self-ligating (ASL) brackets or conventional brackets. To evaluate the mechanical characteristics of the specimens, a three-point bending test was performed. The testing machine vertically applied force on the midpoint of the wire between the central incisor and canine teeth to obtain 2 and 4mm of deflection. The force level at maximum deflection and characteristics of plateau (the average plateau load and the plateau length) were recorded. Two-way ANOVA and Tukey's test were used at P <0.05 level of significance. RESULTS Force level at maximum deflection and plateau length were significantly affected by the amount of deflection. The type of archwires and brackets had significant effects on force level at maximum deflection, and plateau length. However, the bracket type had no significant effect on the average plateau force. CONCLUSION With any type of brackets in deflections of 2 and 4mm, MSNT wire exerted the lowest while NiTi wire exerted the highest force level at maximum deflection and plateau phase. The force level at maximum deflection and the plateau length increased with raising the amount of primary deflection; however the average plateau force did not change significantly.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Deflection Evaluation of Thermoactivated Nickel-Titanium Archwires after Heat Treatment on their Distal Ends.

OBJECTIVE This study evaluated in vitro the mechanical changes of 0.018" (0.45 mm) and 0.016 × 0.022" (0.40 × 0.55 mm) thermoactivated nickel-titanium archwires subjected to heat treatment on their distal ends. MATERIALS AND METHODS Ten archwires in diameters 0.018" and 0.016 × 0.022" by different manufacturers Ormco, Morelli, Orthometric and Unitek were tested. Each tested archwire had an ex...

متن کامل

Force-deflection properties of initial orthodontic archwires.

AIM This in vitro study measured the force-deflection behavior of selected initial alignment archwires by conducting three-point bending tests under controlled conditions. The study tested four wire designs: multistranded stainless steel, conventional stainless steel, superelastic nickel-titanium, and thermoactivated nickel-titanium archwires. METHOD The wires (n = 15) were ligated into stain...

متن کامل

The effect of fluoride exposure on the load-deflection properties of superelastic nickel-titanium-based orthodontic archwires.

BACKGROUND It has been demonstrated that fluoride prophylactic agents may cause hydrogen absorption in NiTi wires and degrade their mechanical properties. AIMS To investigate the effect of a fluoride mouthwash on load-deflection characteristics of three types of nickel-titanium-based orthodontic archwires. METHODS Twenty maxillary 0.016 inch round specimens from each of the single-strand Ni...

متن کامل

Mechanical Properties of Copper-Nickel-Titanium Archwires

MECHANICAL PROPERTIES OF COPPER-NICKEL-TITANIUM ORTHODONTIC WIRES Margaret Rosen, D.M.D. Marquette University, 2016 Introduction: The initial phase of orthodontic therapy relies on flexible wires, usually composed of a nickel-titanium alloy, to apply a substantially constant load during tooth movement. Copper has been added to nickel-titanium archwires, resulting in an alloy with potential clin...

متن کامل

Comparison of the superelasticity of different nickel–titanium orthodontic archwires and the loss of their properties by heat treatment

The aim of this work is to describe and compare mechanical properties of eight widely used nickel-titanium orthodontic wires under uniform testing conditions and to determine the influence of the heat treatments on the loss of the superelasticity. Ten archwires from two batches from eight different manufacturers were evaluated. A three-point bending test was performed, in accordance with ISO 15...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of dentistry

دوره 12 9  شماره 

صفحات  -

تاریخ انتشار 2015