Growth and Magnetic Oscillatory Exchange Coupling of Mn/Fe(001) and Fe/Mn/Fe(001)
نویسندگان
چکیده
The magnetic ordering and the interlayer exchange coupling in Mn and Fe/Mn wedge structures grown epitaxially on Fe(001) whisker substrates were investigated using scanning electron microscopy with polarization analysis (SEMPA). In bare Mn/Fe(001) samples, the magnetization of the top Mn layer is collinear with the Fe magnetization, and oscillates between ferromagnetic and antiferromagnetic alignment as the Mn thickness increases. The period of the oscillation is two layers of Mn, consistent with the growth of an antiferromagnetic Mn wedge. The bare Mn behaves very much like antiferromagnetic Cr, however the magnetic coupling in the Fe/Mn/Fe(001) sandwich structures is very different. For Mn thicknesses greater than four layers, the coupling between the top Fe layer and the Fe whisker substrate is not collinear. Between 4 to 8 layers of Mn, the direction of the top Fe in-plane magnetization lies at an angle of 60° to 80° relative to the magnetization of the Fe substrate. Beginning at the 9 Mn layer, the direction of the coupling oscillates, with a 2 layer period, between 90 φ and 90 + φ, where φ is sample dependent. Values of φ between 10° to 30° were observed.
منابع مشابه
Spin configuration in a frustrated ferromagnetic/antiferromagnetic thin film system
We have studied the magnetic configuration in ultrathin antiferromagnetic Mn films grown around monoatomic steps on an Fe(001) surface by spin-polarized scanning tunneling microscopy/spectroscopy and ab-initio-parametrized self-consistent real-space tight binding calculations in which the spin quantization axis is independent for each site thus allowing noncollinear magnetism. Mn grown on Fe(00...
متن کاملCoupling of Fe and uncompensated Mn moments in exchange-biased Fe/MnPd
A bilayer exchange-bias system composed of Fe/MnPd is investigated using x-ray magnetic circular dichroism XMCD and soft x-ray resonant magnetic reflectometry XRMR . The absorption and XMCD data at the Fe L and Mn L edges are used to derive the optical and magneto-optical properties of the individual layers. Then the structural and magnetic depth profiles of the sample are obtained from XRMR. F...
متن کاملEnergetics of 3d Impurities on the (001) Surface of Iron
Motivated by recent STM results for Cr on Fe(001) we present a detailed ab-initio study of the alloying process in the dilute limit for 3d atoms on the Fe(001) surface. The calculations are based on local density functional theory and apply a KKR{Green's function method for impurities on surfaces. For practically all 3d transition metal impurities on Fe(001) we nd a strong tendency for a direct...
متن کاملFirst-principles investigation of the stability of 3d monolayerÕFe„001... against bilayer formation
Based on the full-potential linearized augmented plane-wave method combined with the generalized gradient approximation, we determine the ground-state spin configurations and the total energies of 3d transitionmetal monolayer and bilayer films on Fe~001! within the c(232) unit cell. We find by energy analysis that V, Cr, and Mn layers prefer the layered antiferromagnetic coupling, and Fe, Co, a...
متن کاملStep-induced frustration of antiferromagnetic order in Mn on Fe(001).
We studied the spin arrangement in ultrathin antiferromagnetic Mn films in contact with a ferromagnetic Fe(001) substrate using spin-polarized scanning tunneling microscopy. Mn shows a layerwise antiferromagnetic order on Fe(001). In regions where Mn overgrows Fe steps, a frustration of the antiferromagnetic order occurs which is similar to a 180 degrees domain wall. This topologically enforced...
متن کامل