This paper deeply analyzes the main factors of the dissolved problems arising in the process of aluminum alloy hard anodizing, combined with the specific problems occurring in production practice, introduces in detail the method and thought to analyze and investigate the causes of dissolving, and puts forward targeted improvement technology. This paper is practically instructive and significant for the production practice to effectively solve the problems of the dissolved situations arising in the process of tube parts hard anodizing.
منابع مشابه
Fast Anodizing of Aluminum Piston Heads
Hard anodizing of aluminum piston heads for internal combustion engines Is usually performed by immersion, with a time ranging from 40 to 50 minutes. This paper wii i present a new process, based on specially adapted hydrodynamics of the electrolyte, applying electrolysis parameter values outside the usual range and which greatly reduce the treatment time. In addition to applications to other c...
متن کاملEFFECT OF MULTI-STEP ANODIZING METHODS ON THE OPTICAL ABSORPTION OF BLACK COATINGS ON 2024 ALUMINUM ALLOY
Development of materials with the ideal black body absorption spectrum are of great interest. Such materials could improve the efficiency of solar cells, and passive cooling and heat transfer systems as well as the protective and decorative coatings. Fabricating black anodizing coatings is promising for this purpose because they exhibit low light reflection from the surface. Such coatings can ...
متن کاملAnalysis of Surface Roughness and Micro-hardness in Roller Burnishing of Aluminum Alloy 6061
Burnishing is a chip-less finishing process, in which a hard roller or ball presses the surface layer of part to perform plastic deformation in the surface layer and produce improved finish, enhanced hardness and compressive residual stresses on the surface of special materials such as Aluminum and Brass. In the following research, the effect of input parameters such as feed rate, cutting speed...
متن کاملThe effects of anodizing condition and post treatment on the growth of nickel nanowires using Anodic Aluminum Oxide
The effects of anodizing condition and post treatment on the growth of nickel nanowires, were investigated. A two-step anodizing process was applied in phosphoric and oxalic acid solution. Nickel electrochemical plating was applied to fill Anodic Aluminum Oxide (AAO) pores. For pore filling enhancement, AAO surfaces were treated by silver predeposition. After electroplating, aluminum and oxide ...
متن کاملPreparation of SiO2/ZrO2 ceramic nanocomposite coating on Aluminum alloys as metallic part of the photovoltaic cells and study its corrosion behavior.
Nowadays due to water shortage, the use of air humidity as the sustainable solution has been considered by cities located in coastal zones; especially in warm and humid climate. However, the use of air humidity also has its own problems such as corrosion of metal parts in photovoltaic cells that used for energy supplying and they are often made of Aluminum alloy. Therefore different methods suc...
متن کامل