Glycerin-Induced Conformational Changes in Bombyx mori Silk Fibroin Film Monitored by 13C CP/MAS NMR and 1H DQMAS NMR

نویسندگان

  • Tetsuo Asakura
  • Masanori Endo
  • Misaki Hirayama
  • Hiroki Arai
  • Akihiro Aoki
  • Yugo Tasei
چکیده

In order to improve the stiff and brittle characteristics of pure Bombyx mori (B. mori) silk fibroin (SF) film in the dry state, glycerin (Glyc) has been used as a plasticizer. However, there have been very limited studies on the structural characterization of the Glyc-blended SF film. In this study, (13)C Cross Polarization/Magic Angle Spinning nuclear magnetic resonance (CP/MAS NMR) was used to monitor the conformational changes in the films by changing the Glyc concentration. The presence of only 5 wt % Glyc in the film induced a significant conformational change in SF where Silk I* (repeated type II β-turn and no α-helix) newly appeared. Upon further increase in Glyc concentration, the percentage of Silk I* increased linearly up to 9 wt % Glyc and then tended to be almost constant (30%). This value (30%) was the same as the fraction of Ala residue within the Silk I* form out of all Ala residues of SF present in B. mori mature silkworm. The ¹H DQMAS NMR spectra of Glyc-blended SF films confirmed the appearance of Silk I* in the Glyc-blended SF film. A structural model of Glyc-SF complex including the Silk I* form was proposed with the guidance of the Molecular Dynamics (MD) simulation using ¹H-¹H distance constraints obtained from the ¹H Double-Quantum Magic Angle Spinning (DQMAS) NMR spectra.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Preparation and characterization of regenerated Bombyx mori silk fibroin fiber with high strength

Regenerated Bombyx mori silk fibers were spun from hexafluoro-isopropanol solution of silk fibroin sponge in methanol used as a coagulant solvent and then elongated in water. The stress-strain curves of the regenerated fibers changed dramatically depending on the draw ratio and the structure was studied by 13C CP/MAS NMR and X-ray diffraction methods. The patterns of 13C CP/MAS NMR spectra of t...

متن کامل

Effects of pH and calcium ions on the conformational transitions in silk fibroin using 2D Raman correlation spectroscopy and 13C solid-state NMR.

Silk fibroin exists in a number of different states, such as silk I and silk II, with different properties largely defined by differences in secondary structure composition. Numerous attempts have been made to control the transitions from silk I to silk II in vitro to produce high-performance materials. Of all the factors influencing the structural compositions, pH and some metal ions play impo...

متن کامل

Local Structure and Dynamics of Serine in the Heterogeneous Structure of the Crystalline Domain of Bombyx mori Silk Fibroin in Silk II Form Studied by 2D C−C Homonuclear Correlation NMR and Relaxation Time Observation

The crystalline fraction (Cp fraction) of silk fibroin in silk II form from the silkworm Bombyx mori is the classic example of antiparallel β-sheet and consists mainly of Ala, Ser, and Gly. In the C CP/MAS NMR spectrum, the Ala Cβ, Ser Cα, and Ser Cβ peaks are asymmetric, showing the heterogeneous nature of the structure, which is shown to consist of two different packing geometries, denoted do...

متن کامل

The silk proteins, sericin and fibroin in silkworm, Bombyx mori Linn., - a review

The domesticated silkworm, Bombyx mori Linn., a lepidopteran molecular model and an important economic insect that are emerging as an ideal molecular genetic resource for solving a broad range of biological problems. The silkworm, B. mori produces massive amount of silk proteins during the final stage of larval development. These proteins are stored in the middle silk gland and they are dischar...

متن کامل

Near-infrared characterization on the secondary structure of regenerated Bombyx mori silk fibroin.

Several advantages of the near-infrared (NIR) technique in the characterization of the secondary structure of regenerated Bombyx mori silk fibroin are demonstrated. Silk fibroin films with thicknesses ranging from 50 to 300 microm are suitable for the NIR measurement. The bands due to hydrogen-bonded water are independent in the NIR spectra and facilitate our investigation of the amide region. ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره 17  شماره 

صفحات  -

تاریخ انتشار 2016