Evaluation of marginal and internal gap of three-unit metal framework according to subtractive manufacturing and additive manufacturing of CAD/CAM systems
نویسندگان
چکیده
PURPOSE To evaluate the fit of a three-unit metal framework of fixed dental prostheses made by subtractive and additive manufacturing. MATERIALS AND METHODS One master model of metal was fabricated. Twenty silicone impressions were made on the master die, working die of 10 poured with Type 4 stone, and working die of 10 made of scannable stone. Ten three-unit wax frameworks were fabricated by wax-up from Type IV working die. Stereolithography files of 10 three-unit frameworks were obtained using a model scanner and three-dimensional design software on a scannable working die. The three-unit wax framework was fabricated using subtractive manufacturing (SM) by applying the prepared stereolithography file, and the resin framework was fabricated by additive manufacturing (AM); both used metal alloy castings for metal frameworks. Marginal and internal gap were measured using silicone replica technique and digital microscope. Measurement data were analyzed by Kruskal-Wallis H test and Mann-Whitney U-test (α=.05). RESULTS The lowest and highest gaps between premolar and molar margins were in the SM group and the AM group, respectively. There was a statistically significant difference in the marginal gap among the 3 groups (P<.001). In the marginal area where pontic was present, the largest gap was 149.39 ± 42.30 µm in the AM group, and the lowest gap was 24.40 ± 11.92 µm in the SM group. CONCLUSION Three-unit metal frameworks made by subtractive manufacturing are clinically applicable. However, additive manufacturing requires more research to be applied clinically.
منابع مشابه
The evaluation and comparison of marginal adaptation in metal ceramic and all ceramic restorations fabricated by two methods: CAD/CAM and conventional
Introduction: Marginal fit is a key factor for long term clinical success through any dental restorations. Poor marginal adaptation causes cement dissolution. This can lead to dental caries, gingival irritation, periodontal diseases, and finally treatment failure. The aim of this study was measurement and comparison of marginal gap quantities in metal ceramic and all ceramic dental restorations...
متن کاملInternal and Marginal Fit of Modern Indirect Class II Composite Inlays
Introduction: This in vitro study investigates the marginal and internal fit of indirect class II composite restorations. Two different processes for chair-side restorations were compared. In group A, the restorations were fabricated using CAD/CAM technology (Cerec, Sirona, Germany, Bernsheim) and in group B they were made by hand (GrandioSO Inlay System, VOCO GmbH, Germany, Cuxhaven). Methods:...
متن کاملمقایسه گپ مارژینال فریم ورکهای زیرکونیایی متکی بر ایمپلنت دو سیستم CAD/CAM
Background and Aims: Marginal accuracy is a crucial factor influencing the clinical long-term reliability of implant-supported fixed dental prostheses (FDPs). The aim of this in vitro study was to evaluate the marginal fit of three-unit zirconia bridge frameworks fabricated using two different computer-aided design (CAD)/ computer-aided manufacturing (CAM) systems (AmannGirrbach and Zirkonzahn...
متن کاملMarginal fit of anterior 3-unit fixed partial zirconia restorations using different CAD/CAM systems
PURPOSE Few studies have investigated the marginal accuracy of 3-unit zirconia fixed partial dentures (FPDs) fabricated by computer-aided design/computer-aided manufacturing (CAD/CAM) system. The purpose of this study was to compare the marginal fit of zirconia FPDs made using two CAD/CAM systems with that of metal-ceramic FPDs. MATERIALS AND METHODS Artificial resin maxillary central and lat...
متن کاملClassifications and Properties of Materials for Chairside Computer-Aided Design/Computer-Aided Manufacturing Dentistry: A Review
Background and Aim: Chairside computer-aided design/computer-aided manufacturing (CAD/CAM) systems have become considerably more accurate, reliable, efficient, fast, and prevalent since 1985 when CEREC was introduced. The inceptive restorative material option for chairside CAD/CAM restorations was limited to ceramic blocks. Today, restorative material options have been multiplied and include me...
متن کامل