Effect of Different Luting Agents on the Retention of Lithium Disilicate Ceramic Crowns
نویسندگان
چکیده
No studies are available that evaluate the retention of disilicate crowns according to different cementation procedures. The purpose of this study was to measure the retention of lithium disilicate crowns cemented using two different cementation systems. Twenty extracted mandibular premolars were prepared. Anatomic crowns were waxed and hot pressed using lithium disilicate ceramic. Teeth were divided into two groups (n = 10): (1) self-curing luting composite and (2) glass-ionomer cement (GIC). After cementation, the crowns were embedded in acrylic resin block with a screw base. Each specimen was pulled along the path of insertion in Universal Testing Machine. Failure load in Newtons (N) and failure mode were recorded for each specimen. Failure mode was classified as decementation or fracture. Failure load data were analyzed using one-way analysis of variance (ANOVA). Failure modes were compared using Pearson's Chi-square test. Mean failure load was 306.6(±193.8) N for composite group and 94.7(±48.2) N for GIC group (p = 0.004). Disilicate crown cemented with luting composite most often failed by fracture; otherwise, crown cemented with glass-ionomer cement most often failed by decementation (p = 0.02). Disilicate full crown cemented with luting composite showed higher failure load compared with conventional cementation with glass-ionomer cement.
منابع مشابه
Effect of adhesive luting on the fracture resistance of zirconia compared to that of composite resin and lithium disilicate glass ceramic
OBJECTIVES The purpose of this study was to evaluate the effect of adhesive luting on the fracture resistance of zirconia compared to that of a composite resin and a lithium disilicate glass ceramic. MATERIALS AND METHODS The specimens (dimension: 2 mm × 2 mm × 25 mm) of the composite resin, lithium disilicate glass ceramic, and yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) were p...
متن کاملFracture resistance of aluminium oxide and lithium disilicate-based crowns using different luting cements: an in vitro study.
AIM The aim of this study was to investigate the fracture resistance of two types of ceramic crowns cemented with two different cements. METHODS AND MATERIALS Forty premolar crowns were fabricated using lithium-disilicate (IPS Empress-2) and glass-infiltrated aluminium-oxide (In-Ceram) ceramic systems. The crowns were divided into four groups (n=10) with Group 1 (IPS Empress-2) and Group 2 (I...
متن کاملThe Effect of Lithium Disilicate Ceramic Thickness and Translucency on Shear Bond Strength of Light-cured Resin Cement
Introduction: To achieve acceptable clinical performance, a ceramic veneer must be bonded to enamel by well-polymerized resin cement. Among different factors, thickness and translucency of the ceramic may affect the resin cement polymerization. Thus, the current study evaluated the effect of the thickness and translucency of lithium disilicate ceramic on light-cured resin cement bond strength t...
متن کاملEffect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown
This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...
متن کاملSilanization effect on microtensile bond strength of a self-adhesive luting material to a disilicate- based glass ceramic
Introduction: The rehabilitation of teeth by means of ceramic indirect restorations has been widely performed. Previous studies has shown the effectiveness of silane coupling agents on improving the bond strength of the adhesion of resin cements to ceramics; however, some studies question the use of silane. Objective: To evaluate the effect of silane application on the microtensile bond strengt...
متن کامل