The photochemical instability of CdSe nanocrystals coated by hydrophilic thiols was studied nondestructively and systematically in water. The results revealed that the photochemical instability of the nanocrystals actually included three distinguishable processes, namely the photocatalytic oxidation of the thiol ligands on the surface of nanocrystals, the photooxidation of the nanocrystals, and the precipitation of the nanocrystals. At first, the thiol ligands on the surface of a nanocrystal were gradually photocatalytically oxidized using the CdSe nanocrystal core as the photocatalyst. This photocatalytic oxidation process was observed as a zero-order reaction in terms of the concentration of the free thiols in the solution. The photogenerated holes in a nanocrystal were trapped onto the thiol ligands bound on the surface of the nanocrystal, which initiated the photooxidation of the ligands and protected the nanocrystal from any photooxidation. After nearly all of the thiol ligands on the surface of the nanocrystals were converted into disulfides, the system underwent several different pathways. If the disulfides were soluble in water, then all of the disulfides fell into the solution at the end of this initial process, and the nanocrystals precipitated out of the solution without much variation over their size and size distribution. When the disulfides were insoluble in water, they likely formed a micelle-like structure around the nanocrystal core and kept it soluble in the solution. In this case, the nanocrystals only precipitated after severe oxidation, which took a long period of time. If the system contained excess free thiol ligands, they replaced the photochemically generated disulfides and maintained the stability and solubility of the nanocrystals. The initiation stage of the photooxidation of CdSe nanocrystals themselves increased as the thickness and packing density of the ligand shell increased. This was explained by considering the ligand shell on the surface of a nanocrystal as the diffusion barrier of the oxygen species from the bulk solution into the interface between the nanocrystal and the surface ligands. Experimental results clearly indicated that the initiation stage of the photooxidation was not caused by the chemical oxidation of the system kept in air under dark conditions or the hydrolysis of the cadmium-thiol bonds on the surface of the nanocrystals, both of which were magnitudes slower than the photocatalytic oxidation of the surface ligands if they occurred at all. The results described in this contribution have already been applied for designing new types of thiol ligands which dramatically improved the photochemical stability of CdSe nanocrystals with a ligand shell that is as thin as approximately 1 nm.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Bioactivation and cell targeting of semiconductor CdSe/ZnS nanocrystals with phytochelatin-related peptides.

Synthetic phytochelatin-related peptides are used as an organic coat on the surface of colloidal CdSe/ZnS semiconductor nanocrystals synthesized from hydrophobic coordinating trioctyl phosphine oxide (TOPO) solvents. The peptides are designed to bind to the nanocrystals via a C-terminal adhesive domain. This adhesive domain, composed of multiple repeats of cysteines pairs flanked by hydrophobic...

متن کامل

Synthesis and Properties of Biocompatible Water-Soluble Silica-Coated CdSe/ZnS Semiconductor Quantum Dots†

We describe the synthesis of water-soluble semiconductor nanoparticles and discuss and characterize their properties. Hydrophobic CdSe/ZnS core/shell nanocrystals with a core size between 2 and 5 nm are embedded in a siloxane shell and functionalized with thiol and/or amine groups. Structural characterization by AFM indicates that the siloxane shell is 1-5 nm thick, yielding final particle size...

متن کامل

Characterization of CdSe Nanocrystals and their Interaction with Micellar Aggregates by Means of Capillary Electrophoretic Techniques

Stable water soluble surfactant coated CdSe nanocrystals with trioctylphosphine (TOP) were obtained by a process of dynamic surface coating with cationic, anionic, and non-ionic surfactants. The surfactant-coated CdSe/TOP nanocrystals were characterized by complementary techniques of UV-VIS and photo-luminescence spectrophotometry, as well as by means of a capillary zone electrophoretic techniq...

متن کامل

Ligand-dependent blinking of zinc-blende CdSe/ZnS core/shell nanocrystals.

Blinking of zinc-blende CdSe/ZnS core/shell nanocrystals are studied as a function of surface passivating ligands. Organic-soluble CdSe/ZnS core/shell nanocrystals are prepared by colloidal synthesis free of trioctylphosphine oxide and converted into water-soluble ones by ligand exchange with three different hydrophilic thiols, 2-aminoethanethiol, 3-mercapto-1-propanol, and 3-mercaptopropionic ...

متن کامل

Solvent-like ligand-coated ultrasmall cadmium selenide nanocrystals: strong electronic coupling in a self-organized assembly.

Strong inter-nanocrystal electronic coupling is a prerequisite for delocalization of exciton wave functions and high conductivity. We report 170 meV electronic coupling energy of short chain poly(ethylene glycol) thiolate-coated ultrasmall (<2.5 nm in diameter) CdSe semiconductor nanocrystals (SNCs) in solution. Cryo-transmission electron microscopy analysis showed the formation of a pearl-neck...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of the American Chemical Society

دوره 123 36  شماره 

صفحات  -

تاریخ انتشار 2001