Temperature rise during photo-polymerization under ceramic restorations.

نویسندگان

  • Dimitrios Dionysopoulos
  • Constantinos Papadopoulos
  • Pantelis Kouros
  • Effrosyni Tsitrou
  • Eugenia Koliniotou-Koumpia
چکیده

AIM The aim of this study was to measure the temperature increase induced by various light-curing units during photo-polymerization beneath ceramic restorations. METHODS Three light-curing units were used; a high intensity QTH unit Elipar 2500 and two LED units: Translux Power Blue and Excelled 1400. The 15 ceramic specimens (CEREC Blocks) used in this study were of 2.5 mm thickness, 5 mm wide and 6 mm long and made using a slow speed saw. Using the same slow speed saw the occlusal enamel portion of 15 mandibular third molars was removed and 15 dentin discs of 1 mm height were prepared. The thickness of the luting cement was delimited to 0.5 mm, using a Teflon mold and then brought into contact with the dentin disc. Light-curing time for all the groups was 20 sec. The temperature rise was measured placing underneath the dentin disc a K-type thermocouple wire connected to a data logger. Five measurements were carried out for each group. Statistical analysis was performed using ANOVA (a=0.05). RESULTS The results indicated that there was a lower temperature rise induced from Translux Power Blue than from the other two light-curing units, which did not present statistically significant difference (p<0.05). However, temperature rise from the light-curing units used in this study is lower than 5.5°C, which is the limit of pulpal damage. CONCLUSIONS Within the limitations of this study, although the type and characteristics of light-curing units may affect temperature rise under ceramic restorations, this influence is possibly not of clinical significance.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Temperature Rise during Resin Composite Polymerization under Different Ceramic Restorations

OBJECTIVES The purpose of this study was to measure temperature increase induced by various light polymerizing units during resin composite polymerization beneath one of three types of ceramic restorations. METHODS The resin composite (Variolink II) was polymerized between one of three different ceramic specimens (zirconium oxide, lithium disilicate, feldspathic) (diameter 5 mm, height 2 mm) ...

متن کامل

In vitro comparison of peak polymerization temperatures of 5 provisional restoration resins.

BACKGROUND The heat produced by provisional restoration materials may injure the dental pulp. This study measured and compared peak temperatures during polymerization of 5 materials used in the fabrication of provisional restorations. METHODS The tested materials were 2 self-curing resins (Integrity and Protemp) and 3 dual-cure resins (Iso-Temp, TCB Dual Cure and Provipont DC). A mould the si...

متن کامل

In vitro pulp chamber temperature rise during fabrication of provisional restorations on different types of teeth

Purpose: This in vitro study compared the temperature rise in the pulp chamber during fabrication of provisional resinous restorations on three types of teeth by a direct method. Materials and Methods: The tip of a thermocouple was positioned into the pulp chamber of thirty intact extracted human teeth. Then the teeth were divided into three different tooth groups (incisor, premolar, molar) and...

متن کامل

Temperature changes under demineralized dentin during polymerization of three resin-based restorative materials using QTH and LED units

OBJECTIVES Light-curing of resin-based materials (RBMs) increases the pulp chamber temperature, with detrimental effects on the vital pulp. This in vitro study compared the temperature rise under demineralized human tooth dentin during light-curing and the degrees of conversion (DCs) of three different RBMs using quartz tungsten halogen (QTH) and light-emitting diode (LED) units (LCUs). MATER...

متن کامل

Influence of light curing unit and ceramic thickness on temperature rise during resin cement photo-activation.

The aim of this study was to determine the effect of different ceramic thickness on heat generation during resin cement photo-activation by QTH (quartz-tungsten-halogen), LED (light emitting diode), and PAC (plasma arc-curing) LCUs (light curing units). The resin cement used was Rely X ARC (3M-ESPE), and the ceramic was IPS Empress Esthetic (Ivoclar-Vivadent), of which 0.7-, 1.4- and 2.0-mm thi...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Oral health and dental management

دوره 12 4  شماره 

صفحات  -