PRECISION MEASUREMENT OF EXCESS ENERGY IN ELECTROLYTIC SYSTEM Pd/D/H2SO4 AND INVERSE-POWER DISTRIBUTION OF ENERGY PULSES VS. EXCESS ENERGY

نویسندگان

  • H. Kozima
  • W.-S. Zhang
  • J. Dash
چکیده

Excess energy was measured with a Seebeck envelope calorimeter in an electrolytic system containing a 2 mm diameter Pd tube cathode. After about 50 hours of electrolysis, many power pulses (Pex < ∼0.5 W) and bursts (Pex > ∼0.5 W) of excess power Pex were observed. The distribution of the number of power pulses N(Pex) with definite excess power Pex plotted on a logarithmic scale is expressed as a straight line with a gradient ~ – 2 for Pex < ∼0.5 W showing the typical behavior of the 1/f noise. The distribution for Pex > ∼0.5 W deviates from this regularity. These characteristic behaviors are discussed in relation to complexity in the mechanism of the excess energy generation in the experimental system.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

PRECISION MEASUREMENT OF EXCESS ENERGY IN ELECTROLYTIC SYSTEM Pd/D/H2SO4 AND INVERSE-POWER DISTRIBUTION OF ENERGY PULSES VS

Excess energy was measured with a Seebeck envelope calorimeter in an electrolytic system containing a 2 mm diameter Pd tube cathode. After about 50 hours of electrolysis, many power pulses (Pex < ∼0.5 W) and bursts (Pex > ∼0.5 W) of excess power Pex were observed. The distribution of the number of power pulses N(Pex) with definite excess power Pex plotted on a logarithmic scale is expressed as ...

متن کامل

Seebeck Envelope Calorimetry with a Pd|d2o+h2so4 Electrolytic Cell

Anomalous excess heat in Pd|D2O+H2SO4 electrolytic cells was confirmed using an accurate method of heat measurement, Seebeck Envelope Calorimetry. A cell was placed in the calorimeter, which measures the output heat flux directly and avoids many of the problems other methods have. The maximum excess power thus far was 1.3 W (or 11 W cm3) with input power of 13 W at a current density of 0.4 A c...

متن کامل

Measurements of Excess Heat in the Open Pd|D2O Electrolytic System by the Calvet Calorimetry

Excess heat was observed in the Pd|D2O electrolytic system using a Calvet type microcalorimeter. It was found that the average excess power was 0.025 W over 79 hours period. This result corresponds to a volume excess power of 8.75 W /cm Pd or a surface excess power of 0.044 W /cm Pd, and a specific excess heat of 2.48 MJ/cm Pd or 228 eV/atom Pd. The current density and D/Pd ratio for excess pow...

متن کامل

Ultrasonically-excited electrolysis Experiments at Energetics Technologies

Three electrolysis cells with built-in ultrasonic transmitters were developed by Energetics Technologies. The ultrasonic transmitters induce cavitation in the electrolyte in the vicinity of the palladium cathode for in-situ cleaning and activation of the cathode surface, generation of dislocations, assistance in loading and excitation of the Pd-D system. The ultrasonically assisted electrolysis...

متن کامل

Some Characteristics of Heat Production Using the “cold Fusion” Effect

Additional evidence is presented to show that heat production resulting from the Pons-Fleischmann Effect has a positive temperature coefficient, has a critical onset current density, and originates at the palladium cathode. Introduction The Pons-Fleischmann effect is proposed to produce energy by initiating a fusion reaction between two deuterium atoms within an electrolytic cell. While an unde...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2007