The calcination reaction of limestone (CaCO3) to yield lime (CaO) is at the heart of many industrial applications as well as natural processes. In the recently emerged calcium-looping technology, CO2 capture is accomplished by the carbonation of CaO in a gas-solid reactor (carbonator). CaO is derived by the calcination of limestone in a calciner reactor under necessarily high CO2 partial pressure and high temperature. In situ X-ray diffraction (XRD) has been employed in this work to gain further insight into the crystallographic transformation that takes place during the calcination of limestone under CO2, at partial pressures (P) close to the equilibrium pressure (Peq) and at high temperature. Calcination under these conditions becomes extremely slow. The in situ XRD analysis presented here suggests the presence of an intermediate metastable CaO* phase stemming from the parent CaCO3 structure. According to the reaction mechanism proposed elsewhere, the exothermicity of the CaO* → CaO transformation and high values of P/Peq inhibit the nucleation of CaO at high temperatures. The wt% of CaO* remains at a relatively high level during slow calcination. Two diverse stages have been identified in the evolution of CaO crystallite size, L. Initially, L increases with CaCO3 conversion, following a logarithmic law. Slow calcination allows the crystallite size to grow up from a few nanometers at nucleation up to around 100 nm near the end of conversion. Otherwise, quick calcination at relatively lower CO2 concentrations limits CaO crystallite growth. Once calcination reaches an advanced state, the presence of CaO* drops to zero and the rate of increase of the CaO crystallite size is significantly hindered. Arguably, the first stage in CaO crystallite growth is driven by aggregation of the metastable CaO* nanocrystals, due to surface attractive forces, whereas the second one is consistent with sintering of the aggregated CaO crystals, and persists with time after full calcination is attained. Our analysis shows that the main mechanism responsible for the increase of CaO crystallite size (and thus for undermining the reactivity of the CaO) under high CO2 partial pressure is enhanced aggregation, whereas CaO sintering is relatively less relevant, as would be expected for calcination temperatures well below the Tamman temperature.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Thermal decomposition of dolomite under CO2: insights from TGA and in situ XRD analysis.

Thermal decomposition of dolomite in the presence of CO2 in a calcination environment is investigated by means of in situ X-ray diffraction (XRD) and thermogravimetric analysis (TGA). The in situ XRD results suggest that dolomite decomposes directly at a temperature around 700 °C into MgO and CaO. Immediate carbonation of nascent CaO crystals leads to the formation of calcite as an intermediate...

متن کامل

On the relevant influence of limestone crystallinity on CO2

8 We analyze the role of limestone crystallinity on its CO2 capture performance when subjected 9 to carbonation/calcination cycles at conditions mimicking the Ca-looping (CaL) technology 10 for post-combustion CO2 capture. The behavior of raw and pretreated limestones (milled and 11 thermally annealed) is investigated by means of thermogravimetric analysis (TGA) tests under 12 realistic sorbent...

متن کامل

Effect of dolomite decomposition under CO2 on its multicycle CO2 capture behaviour under calcium looping conditions.

One of the major drawbacks that hinder the industrial competitiveness of the calcium looping (CaL) process for CO2 capture is the high temperature (∼930-950 °C) needed in practice to attain full calcination of limestone in a high CO2 partial pressure environment for short residence times as required. In this work, the multicycle CO2 capture performance of dolomite and limestone is analysed unde...

متن کامل

CO2 Capture Performance Using Biomass-templated Cement-supported Limestone Pellets

Synthetic biomass-templated cement-supported CaO-based sorbents were produced by granulation process for high-temperature post-combustion CO2 capture. Commercial flour was used as the biomass and served as a templating agent. The investigation of porosity showed that the pellets with biomass or cement resulted in enhancement of porosity. Four types of sorbents containing varying proportions of ...

متن کامل

Sorbent attrition in a carbonation/calcination pilot plant for capturing CO2 from flue gases

There is increasing interest in CO2 looping cycles that involve the repeated calcination and carbonation of the sorbent as a way to capture CO2 from flue gases during the carbonation step and the generation of a pure stream of CO2 in the oxyfired calcination step. In particular, attrition of the material in these interconnected fluidized bed reactors is a problem of general concern. Attrition o...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Physical chemistry chemical physics : PCCP

دوره 17 34  شماره 

صفحات  -

تاریخ انتشار 2015