INTRODUCTION Concerns regarding UHMWPE wear particle induced osteolysis [1] have led to investigations of alternative bearing materials. Carbon-fibre reinforced poly-ether-ether-ketone (CFR-PEEK) has been shown in animal studies to have a similar biological activity to UHMWPE [2], whilst hip and knee configurations incorporating this polymer display reduced wear rates when compared with conventional polyethylene [3]. The aim of this study was to investigate the wear performance of a ceramic-on-CFR PEEK THR through a simulator study combined with wear debris analysis and compare these to wear results from CoCr-onUHMWPE THR which had previously been reported [4].

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Wear of ceramic-on-carbon fibre reinforced PEEK hip replacements

Total hip replacement has been a successful surgical intervention for many years. However, concerns regarding UHMWPE wear particle induced osteolysis [1], have led to alternative bearing materials to be sought. Carbon-fibre reinforced poly-ether-ether-ketone (CFR-PEEK) is a fibre-reinforced polymer which has shown reduced wear in hip and knee configurations compared with conventional polyethyle...

متن کامل

Investigation of Wear Behavior of Biopolymers for Total Knee Replacements Through Invitro Experimentation

The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR  is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...

متن کامل

The wear properties of CFR-PEEK-OPTIMA articulating against ceramic assessed on a multidirectional pin-on-plate machine.

In an attempt to prolong the lives of rubbing implantable devices, several 'new' materials have been examined to determine their suitability as joint couplings. Tests were performed on a multidirectional pin-on-plate machine to determine the wear of both pitch and PAN (polyacrylonitrile)-based carbon fibre reinforced-polyetheretherketone (CFR-PEEK-OPTIMA) pins articulating against both BioLox D...

متن کامل

Are PEEK-on-Ceramic Bearings an Option for Total Disc Arthroplasty? An In Vitro Tribology Study

BACKGROUND Most contemporary total disc replacements (TDRs) use conventional orthopaedic bearing couples such as ultrahigh-molecular-weight polyethylene (polyethylene) and cobalt-chromium (CoCr). Cervical total disc replacements incorporating polyetheretherketone (PEEK) bearings (specifically PEEK-on-PEEK bearings) have been previously investigated, but little is known about PEEK-on-ceramic bea...

متن کامل

PEEK and CFR-PEEK as alternative bearing materials to UHMWPE in a fixed bearing total knee replacement: An experimental wear study

New bearing materials for total joint replacement have been explored as the need to improve longevity and enhance performance is driven by the changing demands of the patient demographic. Carbon-reinforced PEEK has demonstrated good wear characteristics in experimental wear simulation in both simple geometry pin-on-plate studies and in total hip joint replacement. Carbon reinforced PEEK CFR-PEE...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2011