Bulk SmCo5/a-Fe nanocomposite permanent magnets fabricated by mould-free Joule-heating compaction
نویسندگان
چکیده
Bulk SmCo5/a-Fe nanocomposite magnets have been prepared using a Joule-heating compaction technique. Nearly fully dense bulk magnets are obtained by compacting the milled powders under a pressure of 2 GPa at temperatures above 400 C. Structural analysis shows that the grain size of both the SmCo5 and the a-Fe phases is in the range of 10 to 15 nm when the compaction temperature is lower than 500 C, which ensures effective interphase exchange coupling. A further increase in compaction temperature leads to significant grain growth and deterioration of magnetic properties. A maximum energy product of about 18.5 MGOe was obtained in the bulk SmCo5/a-Fe nanocomposite magnets, which is 90% higher than that of the single-phase counterpart prepared under the same conditions. VC 2011 American Institute of Physics. [doi:10.1063/1.3563098]
منابع مشابه
Atom probe study on the bulk nanocomposite SmCo/Fe permanent magnet produced by ball-milling and warm compaction
The microstructure and compositions of the bulk nanocomposite SmCo/Fe permanent magnet were studied using transmission electron microscopy and 3-dimensional atom probe techniques. The excellent magnetic properties were related to the uniform nanocomposite structure with nanometer a-Fe particles uniformly distributed in the SmCo phase matrix. The a-Fe phase contained 26 at% Co, and the SmCo phas...
متن کاملSelf-nanoscaling of the soft magnetic phase in bulk SmCo/Fe nanocomposite magnets
Fabrication of bulk nanocomposite materials, which contain a magnetically hard phase and a magnetically soft phase with desired nanoscale morphology and composition distribution has proven to be challenging. Here we demonstrate that SmCo/Fe(Co) hard/soft nanocomposite materials can be produced by distributing the soft magnetic a-Fe(Co) phase particles homogenously in a hard magnetic SmCo phase ...
متن کاملExchange-coupled nanoscale SmCo/NdFeB hybrid magnets
Nanoscale hybrid magnets containing SmCo5 and Nd2Fe14B hard magnetic phases have been produced via a novel ‘‘in-one-pot’’ processing route. The grain size of the processed bulk composite materials is controlled below 20 nm. The refinement of the nanoscale morphology leads to effective inter-phase exchange coupling that results in single-phase like magnetic properties. Energy product of 14 MGOe ...
متن کاملExplosive shock processing of Pr2Fe14B/ –Fe exchange-coupled nanocomposite bulk magnets
Explosive shock compaction was used to consolidate powders obtained from melt-spun Pr2Fe14B/ –Fe nanocomposite ribbons, to produce fully dense cylindrical compacts of 17–41-mm diameter and 120-mm length. Characterization of the compacts revealed refinement of the nanocomposite structure, with approximately 15 nm uniformly sized grains. The compact produced at a shock pressure of approximately 1...
متن کاملINFLUENCE OF HEATING RATE ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF Fe3B/Nd2Fe14B NANOCOMPOSITE MAGNETS
The nanocomposite magnet, which is composed of exchange coupled nanocrystalline soft (Fe3B, α-Fe) and hard (Nd2Fe14B) magnetic phases, was first reported by Coehoorn et al. [1], and the theoretical basis of it was reported by Kneller and Hawig [2]. Nd-Fe-B based nanocomposite magnet has attracted considerable research interest due to its excellent magnetic properties with relatively low amount ...
متن کامل