Intervention using a novel biodegradable hollow stent containing polylactic acid-polyprolactone-polyethylene glycol complexes against lacrimal duct obstruction disease

نویسندگان

  • Xinyuan Zhan
  • Xin Guo
  • Rong Liu
  • Weikun Hu
  • Lei Zhang
  • Nan Xiang
چکیده

Lacrimal duct obstruction disease (LDOD) is a common ophthalmologic disease. Stent implantation surgery is one of the most effective therapies. In this study, we intended to find out the satisfactory biodegradable stents containing poly-L-lactic acid-polycaprolactone-polyethylene glycol (PLLA- PCL- PEG) complexes for therapeutic application in LDOD. Stents made of PLLA- PCL- PEG complexes in various ratios, were prepared and used in vitro to determine stents with appropriate mechanical properties and shorter range of bio-degradation for study in vivo. Thirty-two rabbits were randomized into eight groups of four eyes each in advance for test in vivo. The selected stents were implanted into the left lacrimal ducts of 16 rabbits and silica gel stents as the control for the other 16 rabbits. At four points in time (1, 4, 10 and 16 weeks after the implantation), weight loss rate (WLR) of the stents was measured and analysed. To access the change of lacrimal duct, fluorescein excretion test, lacrimal duct endoscopy and histopathological testing were conducted. The stent containing PLLA: PCL6: 4+ 15%PEG was selected for study in vivo. Analysis of weight loss rate (WLR), fluorescein excretion test, lacrimal duct endoscopy and histopathological testing indicated that the selected stent was biodegradable and caused minimal stimulation and earlier tissue restoration in the lacrimal epithelium compared with the silica gel stent used as the control. The study results suggest that the PLLA: PCL6: 4+ 15% PEG stent is a satisfactory biodegradable stent as a promising alternative for therapeutic application in LDOD, which showed tissue compatibility, biodegradation and adequate mechanical intensity.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Inhibition of neointima formation after experimental coronary artery stenting: a new biodegradable stent coating releasing hirudin and the prostacyclin analogue iloprost.

BACKGROUND To minimize acute stent thrombosis and development of restenosis, stents coated with biodegradable and nonbiodegradable polymers have been proposed to serve as sustained-release drug carriers. METHODS AND RESULTS In both a sheep and a pig model, we examined the vascular response to standard and high-pressure implantation of coronary Palmaz-Schatz stents coated with a 10-microm laye...

متن کامل

A Simple and Sensitive Method to Quantify Biodegradable Nanoparticle Biodistribution using Europium Chelates

The biodistribution of biodegradable nanoparticles can be difficult to quantify. We report a method using time resolved fluorescence (TRF) from a lanthanide chelate to minimize background autofluorescence and maximize the signal to noise ratio to detect biodegradable nanoparticle distribution in mice. Specifically, antenna chelates containing europium were entrapped within nanoparticles compose...

متن کامل

Nanoparticles of Poly(Lactide-Co-Glycolide)-d-a-Tocopheryl Polyethylene Glycol 1000 Succinate Random Copolymer for Cancer Treatment

Cancer is the leading cause of death worldwide. Nanomaterials and nanotechnologies could provide potential solutions. In this research, a novel biodegradable poly(lactide-co-glycolide)-d-a-tocopheryl polyethylene glycol 1000 succinate (PLGA-TPGS) random copolymer was synthesized from lactide, glycolide and d-a-tocopheryl polyethylene glycol 1000 succinate (TPGS) by ring-opening polymerization u...

متن کامل

Study of PLA Printability with Flexography Ink: Comparison with Common Packaging Polymer

Today, the economic consumption of biodegradable polymers is of capital importance in many applications. One of the most commonly used biopolymers is polylactic acid (PLA). The printability of the biodegradable film has not been fully investigated. This work tested the printability of polylactic acid (PLA) films and compared the print qualities to common packaging films like low density pol...

متن کامل

[Nasolacrimal stent implantation: report of a case].

Epiphora (watering eye) is generally caused by insufficient drainage of tears. The most common cause of epiphora in adults is idiopathic inflammatory obstruction of the nasolacrimal duct. The traditional surgical treatment of nasolacrimal duct obstruction is an external dacryocystorhinostomy, which has an 85% to 95% success rate. To eliminate cutaneus wounds and scarring some techniques were in...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 12  شماره 

صفحات  -

تاریخ انتشار 2017