Effect of zirconia-modified magnesia investment on the casting of pure titanium.
نویسندگان
چکیده
Several investigations have examined magnesia-based investments for pure titanium casting. However, the thermal expansion value was insufficient at low casting temperatures and high interfacial reactivity occurred at high casting temperatures. The purpose of this investigation was to modify a magnesia-based investment by adding a heat-resistant mold material, zirconia, in different ratios to produce a more accurate titanium casting. The thermal expansion value was measured using a new precise automatic laser recording machine and pure titanium was cast using an argon casting machine. The marginal accuracy was measured using a stereomicroscope and the interfacial reactivity of the titanium was evaluated using X-ray diffraction analysis. The results indicate that adding different amounts of zirconia to a magnesia-based investment can increase its thermal expansion value and decrease the interfacial reactivity of the titanium. Maximal thermal expansion in the zirconia-modified investments significantly increased by 5-6 weight % (wt%) and peaked at 1.62% expansion. Selevest with 5 wt% zirconia had the smallest mean marginal discrepancy, 21.70 microm at 750 degrees C. Analysis of variance indicates significant differences in marginal discrepancy between zirconia-modified investments (p < 0.001). Adding zirconia can also decrease the interfacial reactivity of the titanium. The data indicated that proper amounts of zirconia (5-6 wt%) added to a magnesia-based investment can produce a more accurate and less interfacial reactive pure titanium casting.
منابع مشابه
Investigating the effects of Magnesia addition on properties, phase transformation and microstructure of gelcasted Zirconia bodies
Magnesia Partially Stabilized Zirconia (Mg-PSZ) is the best material for casting nozzles used in steelmaking industry due to high melting point, high mechanical strength, high thermal shock resistance, high toughness, chemical stability and neutrality, which these nozzles should be fabricated using cold isostatic pressing (CIP) method, however wet processing methods such as gelcasting can lead ...
متن کاملEffect of magnesia investments in the dental casting of pure titanium or titanium alloys.
For past several years, precious alloys have been gradually replaced by non-precious ones in the dental casting field because of the rising price of dental alloys. In Japan during the past ten years, nickel-chromium alloys have been used extensively for crown or bridge and porcelain-fused-to-metal restorations instead of gold or silver alloys. This tendency seems to be the same all over the wor...
متن کاملEvaluation of the Effect of Zirconia and Titanium Abutments on Microleakage of Implant-Abutment Interface Under Oblique Cyclic Loading In Vitro
Background and Aim: Oral bacteria can proliferate in the implant-abutment interface (IAI) and cause inflammation in the peri-implant tissues and adjacent bone. This study aimed to assess the effect of zirconia and titanium abutments on the microleakage of the IAI under oblique cyclic loading conditions. Materials and Methods: In this in-vitro study, 12 implant-abutment assemblies with zirconia...
متن کاملEnhancement of a titanium denture frame model: mold temperature and spruing factors.
This study evaluated the sensitivity of an experimental model to mold temperature using a two-chamber casting machine and its recommended investment (Exp. 1), and the effect of sprue diameter and length using a one-chamber casting machine and its recommended investment (Exp. 2). Experimental patterns were cast from commercially pure titanium and percentage casting success obtained. Mold tempera...
متن کاملEffect of investment type and mold temperature on casting accuracy and titanium-ceramic bond.
This study evaluated the casting accuracy of crown margins and metal-ceramic shear bond strength (SBS) of pure titanium injected into casting molds made using 2 investment types at 3 mold temperatures. Sixty crown (30-degree beveled finish line) and 60 cylinder (5mm diameter × 8mm high) patterns were divided into 6 groups (n=10), and cast using a phosphate-bonded investment (P) and a magnesium ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- The Kaohsiung journal of medical sciences
دوره 19 3 شماره
صفحات -
تاریخ انتشار 2003