Factors for Consideration in an Open-Flame Test for Assessing Fire Blocking Performance of Barrier Fabrics
نویسندگان
چکیده
The main objective of the work reported here is to assess factors that could affect the outcome of a proposed open flame test for barrier fabrics (BF-open flame test). The BF-open flame test characterizes barrier effectiveness by monitoring the ignition of a flexible polyurethane foam (FPUF) layer placed in contact with the upper side of the barrier fabric, exposed to a burner flame from below. Particular attention is given to the factors that influence the ignitibility of the FPUF, including thermal resistance, permeability, and structural integrity of the barrier fabrics (BFs). A number of barrier fabrics, displaying a wide range of the properties, are tested with the BF-open flame test. Visual observations of the FPUF burning behavior and BF char patterns, in addition to heat flux measurements on the unexposed side of the barrier fabrics, are used to assess the protective performance of the BF specimen under the open flame test conditions. The temperature and heat transfer measurements on the unexposed side of the BF and subsequent ranking of BFs for their thermal protective performance suggest that the BF-open flame test does not differentiate barrier fabrics based on their heat transfer properties. A similar conclusion is reached with regard to BF permeability characterized at room temperature. However, the outcome of this BF-open flame test is found to be heavily influenced by the structural integrity of thermally degraded BF. The BF-open flame test, in its current form, only ignited FPUF when structural failure of the barrier was observed.
منابع مشابه
A review of fire blocking technologies for soft furnishings
Fire barrier fabrics are expected to play an increasingly important role in complying with existing and proposed soft furnishing flammability regulations in the US. The number of commercial fire blocking technologies is large in order to accommodate the vast requirements of the consumers, manufacturers, and regulatory agencies. Generally, highloft, nonwoven fiber battings are used in residentia...
متن کاملProcessing and Characterization of Flame Retardant Cotton Blend Nonwovens for Soft Furnishings to Meet Federal Flammability Standards
Effective from July 1, 2007 it is mandatory that all mattress sets meet the federal flammability standard CFR 1633. It is necessary to impart flame resistance that would provide at least 30min for occupants to escape fire. Changes in the flammability laws are expected on other soft furnishings of sleep products like comforters and pillows. Generally these products are often the first to be engu...
متن کاملEpoxy-based Flame Retardant Nanocomposite Coatings: Comparison Between Functions of Expandable Graphite and Halloysite Nanotubes
Whis work presents a study on the flammability of epoxy coatings containing two types of nano-scale fillers as potential flame retardants: expandable graphite (EG) and halloysite nanotubes (HNTs). Both nanocomposites are prepared by incorporation of the same amount of nanofiller into the epoxy resin for the sake of comparison. Fire retardant nanocomposite coatings are cured through a two-stage ...
متن کاملEnhancement of a Diesel Engine Inlet Port for Pollutant Reduction and Performance Optimization
This research uses computational modeling to explore another method to increase diesel engine performance while maintaining low pollutant emission levels. Previous studies have shown that injection-rate profiles and injector configurations play important roles on the performance and emissions of particulate and NOx in DI diesel engines. Since the most important engine design parameters, includi...
متن کاملPerformance of Flame Retardant Wool Fabric Grafted with Vinyl Phosphate
In this paper, a flame retardant dimethyl-2-(methacryloyloxyethyl) phosphate (DMMEP) was applied to wool fabrics by the graft copolymerization technique initiated with potassium persulfate (KPS) in water media. FTIR and SEM testing were used to explore the grafting evidence on the fiber surface, the SEM results show chemical deposition on the wool fiber surface and the scales could not be seen ...
متن کامل