Evaluation of marginal adaptation of ceramic crowns depending on the marginal design and the addition of ceramic

نویسندگان

  • Edson Hilgert
  • Leonardo Buso
  • Maximiliano Piero Neisser
  • Marco Antonio Bottino
چکیده

Correspondence to: Edson Hilgert Rua Francisco Paes, 31, apto. 22 Centro São José dos Campos CEP 12210-100 São Paulo Brazil Phone: +055 012 39227621 E-mail:[email protected] Abstract This study evaluates the marginal adaptation of ceramic copings front of two finish lines and addition of ceramic. Hence, two master steel dies were milled with all-ceramic crowns preparation, one with a round shoulder finish line margin design, and the other with a deep chamfer. From each one of them, 15 copings were made, and the marginal discrepancy was evaluated in measuring microscope. The ceramic addition was accomplished in both groups with aid of a silicone matrix, and the discrepancies were measured again, obtaining the final mean gap values. The initial measurements resulted means of 44,0μm for deep chamfer and 24,0μm for the round shoulder, and the final measurements were 53,3μm for the deep chamfer and 27,4μm for the round shoulder. The data were submitted to the analysis of variance for verification of influence of the finish lines and application of the ceramic. When analyzed the interaction among the variables it was not observed statistical differences, but when comparing the two types of finish lines or the groups before and after ceramic addition, statistical differences were found. It is was concluded that the round shoulder finish line presents better values of marginal gap than deep chamfer and the addition of ceramic influences in the final gap values of marginal adaptation.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of Different Finishing Lines on the Marginal Fitness of Full Contour Zirconia and Glass Ceramic CAD/CAM Crowns (An in-vitro study)

Purpose: The aim of this study was to evaluate the effect of two gingival finishing lines (90° shoulder and deep chamfer) on the marginal fitness of two types of full anatomic all-ceramic crowns; zirconia crowns (Zikonzhan) and glass ceramic crowns (IPS e-max CAD) milled with CAD/CAM system. Materials and Methods: Two dentoform teeth of left maxillary first molar were prepared with chamfer fini...

متن کامل

The evaluation and comparison of marginal adaptation in metal ceramic and all ceramic restorations fabricated by two methods: CAD/CAM and conventional

Introduction: Marginal fit is a key factor for long term clinical success through any dental restorations. Poor marginal adaptation causes cement dissolution. This can lead to dental caries, gingival irritation, periodontal diseases, and finally treatment failure. The aim of this study was measurement and comparison of marginal gap quantities in metal ceramic and all ceramic dental restorations...

متن کامل

The Effect of Preparation Design on the Marginal Integrity of Monolithic Zirconia Crown

Abstract Background & Aim: Marginal adaptation of full ceramic zirconia restorations are one of the important factors in their long-term success and one of the factors affecting marginal adaptation and their strength is the finish line design.This study was conducted to compare the effect of finishline design on the adaptation of monolithic zirconia crowns. Material and methods: In this in-vitr...

متن کامل

Effect of Core Thickness and Porcelain Sintering on Marginal Adaptation

Background and aim: Marginal adaptation affects the long-term success of full-coverage restorations. This study aimed to assess the effect of porcelain sintering and zirconia core thickness on the marginal adaptation of all-ceramic restorations. Materials and methods: In this in-vitro experimental study, a standard brass die, 7 mm in length and 5 mm in diameter, was fabricated using a milling ...

متن کامل

Effect of Scanner Type on Marginal Adaptation of e.max CAD Crowns

Background and Aim: Marginal adaptation has a significant role in the success and longevity of indirect restorations. This experimental study compared the effect of intraoral and extraoral scanning on the marginal adaptation of the crowns which was made using the CEREC AC system. Materials and Methods: A Typodont maxillary first molar was prepared and served as the master die for an all-cera...

متن کامل

Effect of marginal design on fracture resistance of IPS e.maxall ceramic restorations: Chamfer versus shoulder finish lines

Background and Aim: One of the problems of all ceramic restorations is their risk of fracture due to occlusal loads. The aim of the present study was to compare the effect of two marginal designs (shoulder and chamfer) on the fracture resistance of IPS-emax all ceramic restorations. Materials and Methods: One extracted maxillary first premolar received chamfer 50' marginal preparation (0.8 m...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2004