Correlation between hybrid layer thickness, resin tag length and microtensile bond strength of a self-etching adhesive system.

نویسندگان

  • Vanessa Rahal
  • Fernanda G de Oliveira
  • André L F Briso
  • Paulo H dos Santos
  • Maria L M M Sundefeld
  • Renato H Sundfeld
چکیده

The purpose of this study was to evaluate the correlation between the hybrid layer thickness, resin tag length and resin bond strength of a self-etching adhesive system to sound dentin tissue "in vivo". After performing restorative procedures and tooth extractions, ten specimens were sectioned in a mesiodistal direction. One dental section was used for light microscope analysis, in which both the resin tag length and hybrid layer thickness were measured, while the other section was analyzed using a microtensile test (0.5 mm/min). The fractured surface of the latter section was characterized using a stereoscopic magnifying glass (40x magnifcation). The results were subject to statistical analysis using the Pearson Correlation Test (a = 0.05). The hybrid layer thickness, resin tag length and resin bond strength mean values were 2.19 microm (0.34), 4.34 microm (0.28) and 9.73 MPa (5,55), respectively. In addition, correlation tests between the resin tag length and the resin bond strength (r=0.014) and also between the hybrid layer thickness and bond strength (r=0.43), showed no statistically significant correlation. The microtensile bond strength of Adper Prompt L Pop self-etching adhesive system does not depend on hybrid layer thickness or resin tag length.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis of hybrid layer thickness, resin tag length and their correlation with microtensile bond strength using a total etch adhesive to intact dentin.

The objective of this study was to evaluate the use of a two-step total etch and rinse adhesive, the correlation between the hyybrid layer thickness (HL) and bond strength (BS), and between resin tag length (RT) and bond strength in the same teeth, and also to evaluate the fracture patterns of the tested specimens. Ten human molars were used for the restorative procedure and then sectioned in t...

متن کامل

Correlation of the hybrid layer thickness and resin tags length with the bond strength of a self-etching adhesive system.

The objective of this study was to measure the thickness of the hybrid layer (HLT), length of resin tags (RTL) and bond strength (BS) in the same teeth, using a self-etching adhesive system Adper Prompt L Pop to intact dentin and to analyze the correlation between HLTand RTL and their BS. Ten human molars were used for the restorative procedures and each restored tooth was sectioned in mesio-di...

متن کامل

Microtensile Bond Strength of Self-etching Adhesives to Dentin

The aim of this study was to determine microtensile bond strength of two and one-step self-etching adhesive systems to dentin. 25 intact human third molars were used. Flat surfaces of mid-coronal dentin were exposed and the teeth were divided into 5 groups (n=5). Composite build-ups were made using the following self-etching systems / composite materials: 2-step self-etching system Contax / Ecu...

متن کامل

Evaluation of microtensile bond strength of repaired dental resin composite using different surface treatment techniques: A laboratory study

Background and Aims: Today, resin composites are one of the most commonly used materials in restorative dentistry. However, failure in resin treatments is also common due to its chemical nature and its high talent for decay recurrence. According to conservative approaches, "conservative" treatments are more likely to be considered than "Replacement" of damaged remedies. The purpose of this stud...

متن کامل

Effect of moisture and drying time on the bond strength of the one-step self-etching adhesive system

OBJECTIVES To investigate the effect of dentin moisture degree and air-drying time on dentin-bond strength of two different one-step self-etching adhesive systems. MATERIALS AND METHODS Twenty-four human third molars were used for microtensile bond strength testing of G-Bond and Clearfil S(3) Bond. The dentin surface was either blot-dried or air-dried before applying these adhesive agents. Af...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Acta odontologica latinoamericana : AOL

دوره 25 2  شماره 

صفحات  -

تاریخ انتشار 2012