Marginal and internal adaptation of commercially pure titanium and titanium-aluminum-vanadium alloy cast restorations.

نویسندگان

  • Khalid A Al Wazzan
  • Ahmad A Al-Nazzawi
چکیده

AIM The purpose of this in vitro study was to investigate the marginal accuracy and internal fit of complete cast crowns and three-unit fixed partial dentures (FPDs) cast with commercially pure titanium (CPTi) and Titanium-Aluminum-Vanadium alloy (Ti-6Al-4V). METHODS AND MATERIALS CPTi and Ti-6Al-4V alloy were used to cast twelve single crowns and twelve three-unit FPDs. A traveling microscope was used to measure marginal gap and discrepancies in internal fit. Two and one-way analysis of variance (ANOVA) analyses were used to determine the effects of the marginal and internal fit discrepancies. RESULTS The Ti-6Al-4V alloy demonstrated a significantly smaller marginal gap than CPTi (P<0.0001). The recorded marginal discrepancies for both metals were within a clinically accepted range (<100 microm). The single crown fit discrepancy was significantly smaller than the three-unit FPD for both the CPTi and the Ti-6Al-4V alloy (P<0.0001). For the internal fit discrepancy, the occlusal surface showed the greatest gaps. CONCLUSIONS The Ti-6Al-4V alloy demonstrated a better fit than CPTi. Single crowns showed an improved fit when compared with the three-unit FPD. Mid-occlusal internal gap demonstrated greater values than the axial internal gap. CLINICAL IMPLICATIONS This in vitro study suggested marginal fit of complete crowns and three-unit FPDs cast by CPTi or Ti-6Al-4V alloy were within the range of what is clinically acceptable for longevity of restorations.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The influence of commercially pure titanium and titanium-aluminum-vanadium alloy on the final shade of low-fusing porcelain.

AIMS The aims of this study were to investigate the influence of commercially pure titanium (PTi) and titanium-aluminum-vanadium (Ti-6Al-4V) alloys (TiA) on the final shade of low-fusing porcelain bonded to them and to compare the shade changes with those of three conventional metal-ceramic systems. METHODS AND MATERIALS A titanium casting unit was used to cast PTi and Ti-6Al-4V alloy specime...

متن کامل

Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium

In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...

متن کامل

Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium

In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...

متن کامل

Evaluation of hardness and wear resistance of nano-sized titanium-carbide-reinforced commercially cast aluminum alloy matrices

Production of aluminum matrix composites is widespread because these material provide enhanced mechanical properties compared to aluminum. One the most important parameters of metal matrix composite production is uniform distribution of reinforcing nanoparticles in matrices using the stir-casting method. Second is ensuring high wettability, which is determined by evaluating the properties of ma...

متن کامل

A quantitative comparison of machined commercially pure titanium and titanium-aluminum-vanadium implants in rabbit bone.

Screw-shaped implants made from rods of commercially pure titanium (grade 1) and titanium-aluminum-vanadium (grade 5) were machined, and the implant surface structures were numerically described before being placed in rabbit tibiae for healing periods of 1 months, 6 months, and 12 months. Quantitative comparisons of the removal torque (Ncm) necessary to loosen the implants from the bone bed wer...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The journal of contemporary dental practice

دوره 8 1  شماره 

صفحات  -

تاریخ انتشار 2007