Oxidation Resistance of Materials Based on Ti3AlC2 Nanolaminate at 600 °C in Air
نویسندگان
چکیده
The oxidation behavior of Ti3AlC2-based materials had been investigated at 600 °C in static air for 1000 h. It was shown that the intense increase of weight gain per unit surface area for sintered material with porosity of 22 % attributed to oxidation of the outer surface of the specimen and surfaces of pores in the bulk material. The oxidation kinetics of the hot-pressed Ti3AlC2-based material with 1 % porosity remarkably increased for the first 15 h and then slowly decreased. The weight gain per unit surface area for this material was 1.0 mg/cm(2) after exposition for 1000 h. The intense initial oxidation of Ti3AlC2-based materials can be eliminated by pre-oxidation treatment at 1200 °C in air for 2 h. As a result, the weight gain per unit surface area for the pre-oxidized material did not exceed 0.11 mg/cm(2) after 1000 h of exposition at 600 °C in air. It was demonstrated that the oxidation resistance of Ti3AlC2-based materials can be significantly improved by niobium addition.
منابع مشابه
High Temperature Erosion- Oxidation Behavior of Nickel- Based Alloys Containing Mo in Fluidized Bed Waste Incineration
High-temperature erosion-oxidation behavior of nickel-based alloys containing 0-7 wt.% Mo in fluidized bed waste incineration conditions was studied. A stream of hot condensed air with a flow rate of 25 L/min caused hot silica sand (700 °C) mixed with 0.5 wt.% of chloride salts to hit the specimens for 250 h. By removing the erosive factor, the high-temperature oxidation behavior of the alloys ...
متن کاملElectrophoretic deposition of MnCr2O4 coating for solid oxide fuel cell metallic interconnects
In the present study, Mn - Cr spinel powder was synthesized through a solid state reaction. In the next step, the electrophoretic deposition (EPD) method was used to apply the MnCr2O4 spinel, as an oxidation-resistant layer, on SUS 430 stainless steel in a potential of 300 V/cm. The coated and uncoated samples were then pre-sintered in air at 900 °C for 3 h followed by cyclic oxidation at 800 °...
متن کاملOxidation of ZrB2-SiC Composites at 1600 °C: Effect of Carbides, Borides, Silicides, and Chopped Carbon Fiber
The aim of this work is to optimize the oxidation resistance of ZrB2-SiC-based composites with different additives. Effect of nine factors including SiC, Cf, MoSi2, HfB2 and ZrC contents, milling time of Cf (M.t) and SPS parameters such as temperature, time and pressure on oxidation resistance in four levels was investigated. Taguchi design was applied to explore effective parameters for ...
متن کاملCo3O4 spinel protection coating for solid oxide fuel cell interconnect application
In the present study, electrophoretic deposition (EPD) method in different electric fields (30 – 300 V / cm) was used to apply Co3O4 spinel coating to SUS 430 as SOFC interconnect. The coated and uncoated specimens were pre-sintered in air at 800 and 900 °C for 3 h followed by cyclic oxidation at 700 and 800 °C for 500 h, respectively. X-ray diffraction analysis (XRD), Scanning Electron Microsc...
متن کاملThe study of Oxidation Behavior of AISI 439 Steel at the Presence of Manganese Oxides for the Application in Solid Oxide Fuel Cells
Long–term stability and oxidation resistance of AISI 439 ferritic stainless steel used as interconnects in solid oxide fuel cells can be improved by use of a protective coating. In this study the pack cementation method was employed to coat AISI 439 ferritic stainless steel with manganese. Isothermal oxidation was conducted at 800 ºC for 200 hours in static air to investigate the role of coatin...