Soy-Based Adhesive Cross-Linked by Phenol-Formaldehyde-Glutaraldehyde
نویسندگان
چکیده
To prepare a low-formaldehyde soy-based adhesive with good water resistance, phenol-formaldehyde modified with glutaraldehyde (PFG) with lower free phenol and free formaldehyde contents was used to cross-link the soy-based adhesive. The results showed that the mechanical properties and water resistance of plywood prepared with soy-based adhesive with PFG was better than that of plywood with the same amount of phenol-formaldehyde (PF). The reaction between phenol and glutaraldehyde was proved by 13C-NMR. Under the optimized preparation conditions for plywood, that is to say, press temperature 160 ◦C, press time 4 min and resin loading 320 g·m−2, type I plywood could be prepared with 9% PFG as a cross-linker of soy-based adhesive. The Differential Scanning Calorimetry (DSC) result confirmed the cross-linking reaction between soy-based adhesive and PFG or PF. The activation energy of soy-based adhesive with cross-linker PFG was higher than that with PF resin.
منابع مشابه
Screen printed graphite biosensors based on bacterial cells
A microbial biosensor was developed for the determination of phenolic compounds and the measurement was based on oxygen consumption in relation to analyte oxidation. Induced cells of Pseudomonas putida DSM 50026 were immobilised on the surface of SPG electrodes covered with cellulose acetate membrane by means of gelatine which was then cross linked with glutaraldehyde. The systems were calibrat...
متن کاملBiomimetic soy protein nanocomposites with calcium carbonate crystalline arrays for use as wood adhesive.
Despite the biodegradability, non-toxicity, and renewability, commercially available soy protein-based adhesives still have not been widely adopted by industry, partially due to their disappointing performances, i.e., low glue strength in the dry state and no glue strength in the wet state. In this study, biomimetic soy protein/CaCO(3) hybrid wood glue was devised and an attempt made to improve...
متن کاملDevelopment and characterization of groundnut shell lignin modified phenol formaldehyde wood adhesive
Lignin modified phenol formaldehyde wood adhesives have been prepared by replacing phenol with the groundnut shell lignin (GNSL) at varying weight percentages. The optimization of weight percent incorporation of GNSL was carried out in respect to mechanical properties. It was found that a maximum of up to 50 wt.% of phenol in the phenol formaldehyde (PF) adhesive can be substituted by GNSL to o...
متن کاملDevelopment of Formaldehyde-Based Wood Adhesives with Co-Reacted Phenol/Soybean Flour
Ien resins, each with two replicates, were formulated from soy flour hydrolyzates and prepared with two hydrolyzation variables: phenol-to-soy flour ratios (w/w) of 4/4,3/4,2/4, l/4, and O/4 and sodium hydroxide-to-soy flour ratios (w/w) of 0.39 and 0.78. In addition, two commercially available phenol formaldehyde (PF) resins were used in the study as controls. The most ‘interesting result in t...
متن کاملA New Flexible Soy-Based Adhesive Enhanced with Neopentyl Glycol Diglycidyl Ether: Properties and Application
Soy-based adhesives inherently possess low water resistance and brittleness, which limit their application on plywood fabrication. This investigation involves using a long chain cross-linker, neopentyl glycol diglycidyl ether (NGDE), to produce an intrinsic toughening effect to reduce the brittleness and improve the water resistance of a soybean meal–based adhesive. The solids content, viscosit...
متن کامل