Shear bond strength of dental porcelains to nickel-chromium alloys.
نویسندگان
چکیده
The continuous technological advance and increasing availability of new base metal alloys and ceramic systems in the market, coupled to the demands of daily clinical practice, have made the constant evaluation of the bond strength of metal/porcelain combinations necessary. This study evaluated the metal/porcelain shear bond strength of three ceramic systems (Duceram, Williams and Noritake) in combination with three nickel-chromium (Ni-Cr) alloys (Durabond, Verabond and Viron). Thirty cast cylinder specimens (15 mm high; 6 mm in diameter) were obtained for each alloy, in a way that 10 specimens of each alloy were tested with each porcelain. Bond strength was measured with an Emic screw-driven mechanical testing machine by applying parallel shear forces to the specimens until fracture. Shear strength was calculated using the ratio of the force applied to a demarcated area of the opaque layer. Mann-Whitney U test was used for statistical analysis of the alloy/ceramic combinations (p<0.05). Viron/Noritake had the highest shear bond sregnth means (32.93 MPa), while Verabond/Duceram (16.31 MPa) presented the lowest means. Viron/Noritake differed statistically from other combinations (p<0.05). Viron/Duceram had statistically significant higher bond strengths than Verabond/Duceram, Verabond/Williams and Durabond/Noritake (p<0.05). It was also found significant difference (p<0.05) between Verabond/Noritake, Verabond/Duceram and Durabond/Noritake. No statistically significant difference (p>0.05) were observed among the other combinations. In conclusion, the Noritake ceramic system used together with Viron alloy presented the highest resistance to shear forces, while Duceram bonded to Verabond presented the lowest bond strength. Viron/Duceram and Verabond/Noritake provided intermediate results. The combinations between the Williams ceramic system and Ni-Cr alloys had similar shear strengths among each other.
منابع مشابه
Bond strength of three dental porcelains to Ni-Cr and Co-Cr-Ti alloys.
Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cy...
متن کاملShear Bond Strength of Porcelain Veneering to Nickel-Chromium, Chromium-Cobalt, Zirconia and Lithium Disilicate
Background and Aim: High chipping rates of the veneering porcelain in zirconia ce-ramic restorations have been reported in many clinical studies. However, information on the bonding behavior of veneering porcelain to zirconia and lithium disilicate frameworks is limited. The purpose of this study was to evaluate the bond-ing strength of porcelain veneering to zirconia, lithium disilicate, nicke...
متن کاملبررسی مقایسهای استحکام کششی باند فلز- پرسلن در دو آلیاژ بیسمتال
Statement of Problem: One of the greatest problems in metal –ceramic restorations is debonding of porcelain from dental alloys. Production of dental alloys by Iranian companies necessitates the evaluation of physical and handling properties of these products. Purpose: In this study the bond strength between porcelain and two types of base metal alloys, Supercast (with beryllium) and Minalux (wi...
متن کاملComparative Evaluation of Metal-ceramic Bond Strengths of Nickel Chromium and Cobalt Chromium Alloys on Repeated Castings: An In vitro Study
BACKGROUND Recasting the base metal alloys is done as a routine procedure in the dental laboratories whenever there is casting failure or to decrease the unit cost of a fixed partial denture. However, this procedure may affect the metal ceramic bond. Furthermore, it is unclear, as to which test closely predicts the bond strength of metal-ceramic interface. The aim was to compare the bond streng...
متن کاملComparison of the Effect of Nd:YAG Laser and Sandblasting on Shear Bond Strength of a Commercial Ni-Cr Alloy to Porcelain
Introduction: Failures might occur at metal‒porcelain interfaces as a problem with metal‒ceramic restorations even with the application of airborne-particle abrasion technique. This study was undertaken to evaluate the effect of Nd:YAG laser treatment on the bond strength of porcelain fused to metal. Methods: Twenty-four cylindrical specimens (4 mm in diameter and 4 mm in height) were made of ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Brazilian dental journal
دوره 16 3 شماره
صفحات -
تاریخ انتشار 2005