Flame straightening is a common procedure used for repair work in steel components. It is based on heating a local region of the part by means of a flame torch. Due to the obstruction of the heat expansion, upsetting occurs in the work material. During cooling of the squashed zone shrinkage occurs and that is associated with tension forces which lead to the desired deformation. This process is used in railway shell manufacturing to achieve desired undulation levels of the outer shell skin material. The process of flame straightening suffers from several shortcomings that have strong impacts on the quality, safety and on the economy of railway shell construction. In this paper, a study on the oxyacetylene flame heating of 2mm thick corrosion resistant structural steel sheets (Indian Railway Standard Specification No. M 41 (IRS:M – 41)) is carried out. During heating of IRS:M41 structural steel, an exceeding of oxy acetylene pressure, torch nozzle diameter and the holding time have detrimental effects on mechanical and micro structural properties. The relationship between the micro structural features, tensile and yield strength, elongation and Vickers hardness of material at different combinations of the above parameters were analysed and results were correlated. Based on the experimental results, this study reveals the consequences of flame straightening on microstructure and mechanical properties of the work material influenced by oxy acetylene pressure, torch nozzle diameter and the holding time.
منابع مشابه
Effect of heat treatment on microstructural properties of three-layer sheet aluminum magnesium - aluminum - stainless steel
Metal coating, metal materials are of two or more layers. The coating metals are widely used in industry. These sheets or saving performance and cost effective solution or both the user. Performance coating metals according to usage in structural applications, settings thermal expansion of the thermo-mechanical control (thermostat), electrical, magnetic, corrosion resistant, flowering and decor...
متن کاملPattern of Residual Stress in Rail by FEM Analysis and Strain Gage Sectioning Technique
Final step of rail manufacturing is cold rolling straightening process and it hassignificant effects on mechanical properties, straightness, flatness and development of residualstresses. Measurement of residual stresses after straightening process is obligated by railmanufacturing standards. In the present investigation, an attempt has been made to evaluateresidual stresses after straightening ...
متن کاملDevelopment of a Predictive Finite Element Model For Investigation of Phases Behavior After Cold Rolling Process
One of the surface defects that arise in sheet metal working is when the part removes from the die. Since there are no external forces to make this defect, the origin of such fail is known as residual stress. Residual stress can develop in sheet metal forming due to non uniform deformation. In this paper, the workpiece is carbon steel with different volume fractions and arrangement of ferrite ...
متن کاملExperimental Study on Impact Load Resistance of RC Beam with Corroded Reinforcement
In Japan, many concrete bridges along the coastline have suffered corrosion due to the chloride attack from seawater and airborne salt. Therefore, now, several researches on corroded RC structures have been ongoing around the world. Especially, as a basic research, many researchers have studied on the numerical and experimental method to evaluate static load resistant capacity of RC beams with ...
متن کاملThe Effect of Header Geometry on Temperature Distribution in Cold Rolling
The objectives in the cold rolling process include improved sheet surface quality, enhanced steel mechanical strength, and better solidification operations. Given the increasing demand for higher steel...