Friction and wear behaviours of medical grade UHMWPE at dry and lubricated conditions

نویسندگان

  • O. K. Kahyaoglu
  • H. Unal
چکیده

In this investigation the friction and wear performance of GUR 1020 medical grade ultra-high molecular weight polyethylene (UHMWPE) polymer under dry sliding, distilled water and egg albumen lubrication conditions were evaluated. The sliding experiments were carried out on a pin-on-disc tribometer. The contact configuration used was a polymer pin on a rotating AISI 304L stainless steel disc. Wear tests were carried out for 30 min duration at room temperature with 50, 100 and 150 N applied load values and at 0.50, 1.0 and 2.0 m/s sliding speeds condition. The results show that the coefficient of friction for GUR 1020 medical grade UHMWPE polymer is more significantly influenced by applied load and sliding speed values under dry sliding condition rather than lubricant media condition. Furthermore, the coefficient of friction and specific wear rate increases with the increase in applied load and speed values. This increase is much pronounced under dry sliding condition. Moreover, for the range of load and speed values of this study the specific wear rate using egg albumen lubricant registered lower values than that of the distilled water lubricant and the dry conditions. Finally, the specific wear rate values for GUR 1020 medical grade UHMWPE polymer under dry, water lubricant and egg albumen lubricant conditions are at the levels of 8x10 -14 , 1.4x10 -14 and 0.5x10 -14 m 2 /N respectively.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

ÇYMAPE ve PEEK POLİMERLERİNİN KURU ve KAKAO ÇÖZELTİSİ ORTAMLARINDAKİ A INMA ve SÜRTÜNME DAVRANI LARININ ARA TIRILMASI INVESTIGATION OF FRICTION AND WEAR BEHAVIOUR OF UHMWPE AND PEEK POLYMERS UNDER DRY SLIDING AND CACAO LUBRICATED CONDITIONS

The friction and wear performance of ultra high molecular weight polyethylene(UHMWPE) and pure poly-ether-etherketone(PEEK) polymers were comparatively evaluated under dry sliding and cacao drops lubrication. The sliding experiments were carried out on a pin-on-disc tribometer. The contact configuration used was a polymer pin on a rotating stainless steel disc. Wear tests were carried out at ro...

متن کامل

Tribological behaviors of several polymer–polymer sliding combinations under dry friction and oil-lubricated conditions

The friction and wear properties of polyamide 66 (PA66), polyphenylene sulfide (PPS) and polytetrafluoroethylene (PTFE) sliding against hemselves under dry sliding and oil-lubricated conditions were studied by using a pin-on-disc tribometer. The effect of applied load and sliding peed on tribological behaviors of the polymer–polymer sliding combinations under dry sliding and oil-lubricated cond...

متن کامل

Mechanical Application of Lubricated Nano Porous Anodized Aluminium

Today a major environmental problem is global warming that is mainly caused due to exhaust and emission of gases. The only way to reduce their ill-effect is by improvement in fuel efficiency of I.C. engines, where most of the power is lost to overcome the friction. In this work, nanoporous anodized layer is formed on an aluminium substrate surface by anodization. Anodization was carried out at ...

متن کامل

Influence of roughness on contact interface in fretting under dry and boundary lubricated sliding regimes

This paper presents experimental results of wear process under dry and boundary lubricated metallic (AISI 1034/AISI 52100) contacting bodies with different surfaces morphologies subjected to a wide range of kinematic fretting conditions. Analysis of damage mode observed under such fretting conditions is elucidated in context of surfaces morphologies therefore associated with surface manufacturi...

متن کامل

Variation of Friction Factor Through the Gait Cycle in an UHMWPE-CoCrMo Hip Endoprosthesis

* email: [email protected] John Charnley was the first who introduced low friction arthroplasty concept. In November 1962, he implanted a hip prosthesis using a high density polyethylene (HDPE) cup, which articulated with a stainless steel femoral head of 22,25 mm diameter. The principle of the low friction arthroplasty has remained the same ever since. Because HDPE have not a goo...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2012