Bond characteristics of porcelain fused to cast and milled titanium

نویسندگان

  • Karina Andrea Novaes Olivieri
  • Maximiliano Piero Neisser
  • Marco Antônio Bottino
  • Edson Miranda
چکیده

Karina Andrea Novaes Olivieri 1 Maximiliano Piero Neisser 2 Marco Antônio Bottino 2 Milton Edson Miranda 3 1PhD, Post-graduated, Department of Dental Materials and Prosthodontics, Faculty of Odontology of São José dos Campos, UNESP, Brazil and Associated Professor, Department of Prosthodontics, Faculty of Odontology São Leopoldo Mandic – CampinasBrazil. 2PhD, Associated Professor, Department of Dental Materials and Prosthodontics, Faculty of Odontology of São José dos Campos, UNESP, Brazil. 3PhD, Associated Professor, Department of Prosthodontics, Faculty of Odontology São Leopoldo Mandic, Campinas, Brazil.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Cast, milled and EBM-manufactured titanium, differences in porcelain shear bond strength.

The objectives were to analyze the oxide layer generated between titanium and porcelain during firing and compare it in different manufacturing techniques: cast, milled and EBM-technique. Seventy two specimens were manufactured, subdivided according to surface treatment: time of passivation (P) and no time of passivation (NP) before porcelain firing. Specimens from each group were analyzed with...

متن کامل

Treatment Plan For: Single implant crown supported by a pre-fabricated abutment

D6056 prefabricated abutment includes placement D6057 custom abutment includes placement D6058 abutment supported porcelain/ceramic crown D6059 abutment supported porcelain fused to metal crown (high noble metal) D6060 abutment supported porcelain fused to metal crown (predominantly base metal) D6061 abutment supported porcelain fused to metal crown (noble metal) D6062 abutment supported cast m...

متن کامل

Shear bond strengths of veneering porcelain to cast, machined and laser-sintered titanium.

The aim of this study was to compare the shear bond strengths (SBS) of cast, machined, and laser-sintered titanium to dental porcelain. Two kinds of dental porcelains (Titankeramik and Triceram) were applied on cast (Tritan), machined (DC-Titan), and laser-sintered (EOSINT) titanium specimens (n=10). SBS test was conducted, and fracture surface analysis was also performed to determine the failu...

متن کامل

Bond strengths of porcelain to cobalt-chromium alloys made by casting, milling, and selective laser melting.

STATEMENT OF PROBLEM Cobalt-chromium (Co-Cr) alloys have been widely used for metal-ceramic fixed prostheses and can be fabricated using conventionally cast or new computer-aided technology. However, the effect of different manufacturing methods on the metal-ceramic bond strength needs further evaluation. PURPOSE The purpose of this in vitro study was to evaluate the metal-ceramic bond streng...

متن کامل

Cross-sectional TEM analysis of porcelain fused to gold-coated titanium.

This study investigated the interfacial microstructure between gold-coated titanium and low-fusing porcelain. The square surfaces of cast titanium split rods were sputter-coated with gold using a sputter coater at 40 mA for 1,000 seconds. Specimens were prepared for transmission electron microscopy (TEM) by cutting and polishing two pieces of the gold-coated split-rod specimens, which were glue...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2005