In situ investigation of thermally influenced phase transformations in (Pb 0.92 Sr 0.08)(Zr 0.65 Ti 0.35)O3 thin films using micro-Raman spectroscopy and X-ray diffraction.
نویسندگان
چکیده
Thin films of ferroelectric strontium-doped lead zirconate titanate [PSZT, (Pb(0.92)Sr(0.08))(Zr(0.65)Ti(0.35))O(3)] deposited by RF magnetron sputtering have been analyzed by in situ analysis techniques. The in situ techniques employed for this study include micro-Raman spectroscopy and X-ray diffraction (XRD), and variations in thin film structure and orientations for temperatures up to 350 degrees C and 750 degrees C for the respective techniques have been studied. The samples analyzed were PSZT thin films deposited on platinum-coated silicon substrates at either room temperature or at 750 degrees C. In situ measurements using micro-Raman spectroscopy and XRD techniques have been used to identify the Curie point for poly-crystalline PSZT thin films and to determine the temperature-activating significant grain growth for room-temperature-deposited PSZT thin films. To study the presence of hysteresis, analysis was carried out during both temperature ramp-up and ramp-down cycles. Raman measurements showed expected bands (albeit weak), and the in situ measurements have detected variations in the crystal structure of the thin film samples, with negligible variations between the heating and cooling cycles. A combination of the Raman and XRD results has shown that the temperature-activating significant grain growth for the room-temperature-deposited films is about 275 degrees C and the Curie point lies between 325 and 400 degrees C. This relatively high Curie point makes these films suitable for wide temperature range applications.
منابع مشابه
Average and local atomic-scale structure in BaZrxTi(1-x)O3 (x = 0. 10, 0.20, 0.40) ceramics by high-energy x-ray diffraction and Raman spectroscopy.
High-resolution x-ray diffraction (XRD), Raman spectroscopy and total scattering XRD coupled to atomic pair distribution function (PDF) analysis studies of the atomic-scale structure of archetypal BaZrxTi(1-x)O3 (x = 0.10, 0.20, 0.40) ceramics are presented over a wide temperature range (100-450 K). For x = 0.1 and 0.2 the results reveal, well above the Curie temperature, the presence of Ti-ric...
متن کاملLaser Annealing of MOCVD Deposited Ferroelectric SrBi 2 Ta 2 O 9 , Pb ( ZrXTi 1 - X ) O 3 and CeMnO 3 Thin Films
Excimer laser annealing studies were conducted of SrBi2Ta2O9, Pb(ZrxTi1-x)O3 and CeMnO3 thin films. The main incentive was to develop a low temperature process for SrBi2Ta2O9 thin films, which typically require a 750 C anneal to crystallize and achieve optimum ferroelectric properties. The results show that room temperature laser annealing can crystallize SrBi2Ta2O9, with a strong (200) preferr...
متن کاملPb(Zr,Ti)O3 Thin Films on Zirconium Membranes for Micromechanical Applications
An efficient, electrically conductive, chemical barrier for the integration of piezoelectric Pb(Zr,Ti)O3 (PZT) films on reactive metal substrates has been developed, opening new possibilities for PZT integration on micromechanical and semiconductor devices, Very reactive zirconium films have been taken in order to test the quality of the specially designed RuO2/Cr buffer under the condition of ...
متن کاملSol–gel derived Pb(Zr,Ti)O3 thin films: Residual stress and electrical properties
Pb(Zr,Ti)O3 compositions are under investigation for applications that include integrated capacitors, piezoelectric sensors, and actuators. Sol–gel synthesis and spin coating are popular routes to the formation of high quality, dense, crack free, insulating films. However, the electrical properties of the films are often different than those measured for bulk specimens of the same composition. ...
متن کاملProbing fatigue in ferroelectric thin films with subnanometer depth resolution
The authors report the study of polarization fatigue in Pb Zr,Ti O3 PZT ferroelectric thin films using in situ high-resolution grazing incidence x-ray specular reflectivity of synchrotron radiation. The results demonstrate that there is no formation of a region of different electron densities in the film growth direction with subnanometer depth resolution during fatigue. The upper bounds on the...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- IEEE transactions on ultrasonics, ferroelectrics, and frequency control
دوره 56 2 شماره
صفحات -
تاریخ انتشار 2009