STATEMENT OF PROBLEM Patients' demand for tooth-colored restoratives in the posterior region is increasing. Clinicians use universal nanohybrid resin composites for both anterior and posterior regions. There are few published reports comparing fracture toughness of nonohybrids and that of hybrid composite stored wet and dry. OBJECTIVES To investigate the fracture toughness of three nanohybrids compared to that of a hybrid resin composite stored dry or wet up to 60 days, using four-point bending test. MATERIALS AND METHODS Four resin composites were used: three nanohybrids; Filtek Supreme (3M), Ice (SDI), TPH3 (Dentsply) and one hybrid Filtek P60 (3M). For each material, 40 rectangular notched beam specimens were prepared with dimensions of 30 mm × 5mm × 2mm. The specimens were randomly divided into 4 groups (n = 10) and stored at 37ºC either in distilled water or dry for 1 and 60 days. The specimens were placed on the four-point test jig and subjected to force (N) using universal testing machine loaded at a crosshead speed of 0.5mm/min and maximum load at specimen failure was recorded and KIC was calculated. RESULTS Three-way ANOVA showed a significant interaction between all the factors (all p < .0001). Except for TPH3, all tested materials showed significantly higher KIC when stored dry than stored wet (p < 0.05). After 1 day of dry storage, Ice showed the highest KIC (2.04± 0.32) followed by Filtek P60 and the lowest was for Filtek Supreme (1.39± 0.13) The effect of time on fracture toughness was material dependent. CONCLUSIONS Wet storage adversely affected the fracture toughness of almost all materials. Keeping the restoration dry in the mouth may increase their fracture toughness. Therefore, using a coating agent on the surface of restoration may protect them from early water uptake and increase their strength during a time period.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

چقرمگی شکست و تغییر رنگ کامپوزیت‌های رزینی نانوهیبرید در محیط خشک و مرطوب به مدت 60 روز

Background and Aims: Fracture and color change are among the most common causes of clinical failure of resin composite restorations. Therefore, this study aimed to examine the fracture toughness and color changes of 3 Nano-hybrid resin composites in dry and wet conditions. Materials and Methods: Three resin composites were studied. A total of 36 rectangular specimens were prepared for each mat...

متن کامل

بررسی جذب آب، حلالیت و ریزسختی سطحی سه نوع کامپوزیت رزینی نانوهیبرید در طول 60 روز ذخیره در آب

Background and Aims: Microhardness, sorption, and solubility are useful predictors of a resin composite&rsquo;s clinical success. This study aimed to evaluate the effect of 60 days of water storage on the microhardness, sorption, and solubility of 3 commercial nanohybrid resin composites. Materials and Methods: Three nanohybrid composites were evaluated: GC Kalore (GC), Aura (SDI), and G-&aeli...

متن کامل

Investigation of Mode I Delamination Resistance in Inter-ply and Intra-ply Hybrid Composites Reinforced with Basalt/Nylon Woven Fabrics

Due to their sensitivity to impact-induced delamination, woven fabric reinforced polymer composites have limited practical applications. Hybridization of polymer composites has been proposed as a solution to this problem. In this study, the effects of fiber reinforcement type, hybridization method, plies stacking sequence and loading rate on mode I delamination behavior of pure basalt, pure nyl...

متن کامل

Wet/Dry Cycling Durability of Cement Mortar Composites Reinforced with Micro- and Nanoscale Cellulose Pulps

A combination of reinforcements at different levels can have a synergetic effect on the final properties of a composite. The aim of this work was to produce, evaluate, and compare the wet/dry cycling durability of the exposure of cement composites reinforced with conventional pulps at the micro-scale level, with nanofibrillated cellulose fibers at the nano-scale level, and with combinations of ...

متن کامل

Prediction of Mode II of Fracture Toughness in Laminate Composites

In this paper, effects of ply orientation of adjacent plies with (ϕ//θ) interfaces on mode II critical strain energy release rate (fracture toughness) of multidirectional (MD) laminate has been studied. Ply orientation of adjacent plies is one of the most important parameters affects the mode II critical strain energy release rate () in the initiation of the delamination. To  study this paramet...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 4  شماره 

صفحات  -

تاریخ انتشار 2017