Influence of thermal and mechanical load cycling on microtensile bond strengths of total and self-etching adhesive systems.

نویسندگان

  • Fabio Hiroyuki Ogata Mitsui
  • Alessandra Rezende Peris
  • Andrea Nóbrega Cavalcanti
  • Giselle Maria Marchi
  • Luiz André Freire Pimenta
چکیده

This study evaluated the influence of different thermal (TC) and mechanical (MC) cycling protocols on microtensile bond strength (muTBS) to cervical dentin margins of Class II restorations using two total-etch (TE) adhesives and one self-etching (SE) primer. Class II slot cavities were prepared on the mesial surfaces of 168 bovine incisors and were divided into three groups according to the bonding system used: Single Bond, OptiBond Solo Plus and Clearfil SE Bond. All cavities were restored with Filtek Z250 composite. Following restorative procedures, the restored teeth were allocated to seven subgroups (n = 8) according to the thermal/mechanical protocol performed: G1-control (no cycling), G2-100,000 MC, G3-200,000 MC, G4-500,000 MC, G5-100,000 MC+1,000 TC, G6-200,000 MC+1,000 TC, G7-500,000 MC+1,000 TC. TC was performed using 5 +/- 2 degrees C and 55 +/- 2 degrees C baths, with a dwell time of 60 seconds in each bath. MC was achieved with an axial force of 80 N at 2 cycles/second. The restorations were sectioned perpendicular to the cervical bonded interface into two 0.8-1-mm thick slabs. The slabs were trimmed at the interface to obtain a cross-sectional surface area of 0.8-1 mm2. All specimens were then subjected to muTBS (v = 0.5 mm/minute). Fracture mode analysis was performed using SEM. Bond strength mean values (MPa) were analyzed with ANOVA 3-way and Tukey's test (alpha = 5%). Dunnett's test was used to compare tested groups against Control groups of each adhesive system (alpha = 56%). SE primer presented lower mean bond strength values when compared to TE adhesives (p = 0.05). In addition, specimens restored with the SE primer did not resist to the 200,000 and 500,000 MC associated with TC. The application of 100,000 MC did not present a significant decrease in bond strength when compared to the control. Mixed failures were predominant for all groups. The higher the amount of thermal/mechanical cycles, the greater the number of mixed failures and the lower the percentage of adhesive failures.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Strength and Durability of a New Adhesive Bond to Superficial Dentin Using Etch and Rinse and Self-Etch Systems: An In Vitro Study

Background and Aim: Data regarding the efficacy of universal adhesives are limited. This study aimed to assess the durability of a universal adhesive bond to superficial dentin using etch and rinse and self-etch modes. Materials and Methods: In this in vitro, experimental study, 32 sound molars were randomly divided into two groups of Scotchbond Universal adhesive with two-step etch and rins...

متن کامل

Er:YAG pre-treatment for bonding of orthodontic bracket: 1 year of in vitro treatment

OBJECTIVE The aim of this study was to evaluate in vitro bond strength of metal brackets bonded with: total etch, total etch with erbium: yttrium aluminum garnet laser (Er:YAG) and self-etching adhesive systems, submitted to thermal-mechanical cycling, simulating 1 year of orthodontic treatment. MATERIALS AND METHODS For the study, 80 bovine incisors were randomly divided into 3 experimental ...

متن کامل

Influence of adhesive systems on microtensile bond strength of resin-based endodontic sealers to the root dentin

OBJECTIVE The aim of this study was to determine the microtensile bond strength to root dentin of AH Plus™ and EndoREZ® with Clearfil Liner Bond 2V and Optibond Solo™ Plus adhesive systems. STUDY DESIGN The coronal and middle thirds of six single rooted bovine teeth was split longitudinally in a mesio-distal direction. The two halves were joined with AH Plus or EndoREZ, with and without the u...

متن کامل

Effect of high-power LED light curing unit on bond strength of composite resin to dentin

Purpose: This study evaluated the effect of a high-power solid-state light emitting diode (LED) curing unit on the dentin bond strength of a composite resin with self-etching primer adhesives by means of microtensile bond test. Materials and Methods: The flat dentin surfaces of the extracted human molars were prepared. Each surface was treated with either two self-etching adhesive systems (Clea...

متن کامل

Effect of Saliva Contamination and sequencing time of curing the Transbond™ Plus Self Etching Primer on the Shear Bond Strength of Orthodontic Brackets

Abstract Background and aim: Over the years, improvments have been done to simplify clinical bonding procedure. One of these material is Transbond™ Plus Self Etching. The aim of this study was to evaluate the effect of saliva contamination and reusing Transbond™ Plus Self Etching Primer (SEP) on shear bond strength of orthodontic brackets. Materials and Methods: Fifty premolars divided into fiv...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Operative dentistry

دوره 31 2  شماره 

صفحات  -