Protocols for sodium ascorbate application on intracoronary dentin bleached with high-concentrated agent
نویسندگان
چکیده
Purpose Composite resin restorations are normally replaced after the internal bleaching of endodontically treated-teeth because the bleaching agent does not alter the color of the restorative material. This study evaluated the effect of 10% sodium ascorbate (SA) applied at different protocols on bleached dentin. Materials and Methods One-hundred slabs of intracoronary bovine dentin were divided into 5 groups: 2 controls-GI without bleaching (positive), GII bleached with 35% hydrogen peroxide (HP) (negative); and 3 experimentals - GIII. 35% HP + SA at protocol 1 (dripping, washing and drying the solution), GIV. 35% HP + SA at protocol 2 (dripping and aspirating the solution) and GV. 35% HP + SA at protocol 3 (dripping, rubbing and aspirating the solution). Sixty fragments were restored and subjected to shear bond strength test (n = 12). Forty fragments (n = 8) were prepared for chemical analysis (energy dispersive X-ray spectrometry) and surface morphology (scanning electron microscopy). Data were analyzed by ANOVA and Tukey test (P < 0.05). Results GI (3.169 ± 1.510a) had the highest means values, similar to GIV (2.752 ± 0.961a) and GV (2.981 ± 1.185a) (P < 0.05). Inferior values were obtained in GII (1.472 ± 0.342b) and GIII (2.037 ± 0.742ab) had intermediate values (P > 0.05). Oxygen concentration was reduced in groups treated with SA, and the surface exhibited residual granules of the solution. Conclusion The 10% SA solution reestablishes the bond strength of restorative material to bleached dentin, especially if active protocols of application and aspiration were used.
منابع مشابه
Shear Bond Strength of Two Types of Glass Ionomer to Bleached Dentin: Effect of Delayed Bonding and Antioxidant Agent
BACKGROUND Studies have shown a reduction in bond strength of composites and glass ionomer to bleached enamel and dentin. Several methods have been proposed to reverse compromised bond strength. OBJECTIVE The aim of this study was to evaluate the effect of delayed bonding and application of antioxidant agent on the bond strength of reinforced self-cured (Fuji IX) and light-cured glass ionomer...
متن کاملBond Strength of Composite Resin to Bleached Dentin: Effect of Using Antioxidant Versus Buffering Agent
OBJECTIVE Application of sodium ascorbate as an antioxidant and calcium hydroxide as a buffering agent following intracoronal bleaching has been recommended. The aim of this study was to investigate the effect of using the mentioned materials on shear bond strength of composite resin to the bleached dentin. MATERIALS AND METHODS In this in vitro investigation, sixty human sound premolars were...
متن کاملTime of Application of Sodium Ascorbate on Bonding to Bleached Dentin
This study examined the effects of different application times of sodium ascorbate (SA) on the bond strength of composite resin to bleached dentin. Specimens with an exposed dentin surface were divided into 3 groups according to the type of bleaching agent used: Group A, mixture of sodium perborate (SP) and distilled water (DW); Group B, mixture of SP and hydrogen peroxide (HP); control group, ...
متن کاملPost-bleaching application of an antioxidant on dentin bond strength of three dental adhesives
BACKGROUND Antioxidizing agents have recently been suggested to compensate decreased bond strength of resin materials to bleached tooth tissues. This study compared the shear bond strength (SBS) of three different adhesives on bleached dentin immediately after bleaching, bleached/delayed for 1 week, and bleached/applied antioxidizing agent. MATERIALS AND METHODS The dentinal surfaces of 132 i...
متن کاملBonding Effectiveness of Universal Adhesive to Intracoronal Bleached Dentin Treated with Sodium Ascorbate.
This study evaluated the effect of restorative protocol with sodium ascorbate on the shear bond strength (SBS) of a universal adhesive to intracoronal bleached dentin. One hundred-and-twenty bovine dentin fragments were randomly divided into 12 groups (n=10), according to the bleaching procedure (unbleached and bleached) and restorative protocol (no treatment, 10% sodium ascorbate -10SA, 35% so...
متن کامل