Effect of adhesive primers on bonding strength of heat cure denture base resin to cast titanium and cobalt-chromium alloy
نویسندگان
چکیده
STATEMENT OF PROBLEM The poor chemical bonding of a denture base resin to cast titanium framework often introduces adhesive failure and increases microleakage. PURPOSE This study evaluated the shear bond strengths of a heat cure denture base resin to commercially pure titanium, Ti-6Al-4V alloy and a cobalt-chromium alloy using two adhesive primers. MATERIAL AND METHODS Disks of commercially pure titanium, Ti-6Al-4V alloy and a cobalt-chromium alloy were cast. Specimens without the primer were also prepared and used as the controls. The shear bond strengths were measured on a screw-driven universal testing machine. RESULTS The primers significantly (P < .05) improved the shear bond strengths of the heat cure resin to all metals. However, the specimens primed with the Alloy primer® (MDP monomer) showed higher bond strength than those primed with the MR bond® (MAC-10 monomer) on titanium. Only adhesive failure was observed at the metal-resin interface in the non-primed specimens, while the primed specimens showed mixed failure of adhesive and cohesive failure. CONCLUSIONS The use of appropriate adhesive metal primers makes it possible not only to eliminate the need for surface preparation of the metal framework before applying the heat cure resins, but also reduce the need for retentive devices on the metal substructure. In particular, the Alloy primer®, which contains the phosphoric acid monomer, MDP, might be clinically more acceptable for bonding a heat cure resin to titanium than a MR bond®, which contains the carboxylic acid monomer, MAC-10.
منابع مشابه
Bonding properties of heat-polymerized denture base resin to Ti-6Al-7Nb alloy.
The purpose of this study was to evaluate the shear bonding strength and leakage of heat-polymerized denture base resin to titanium-aluminum-niobium (Ti-6Al-7Nb) and cobalt-chromium (Co-Cr) castings using four adhesive systems; three adhesive primers (Metal Primer II, Metal Link, MR. Bond) and one heat-polymerized adhesive resin containing 4-META (Metadent). The resin tab was heat-polymerized d...
متن کاملShear bond strengths of polymethyl methacrylate to cast titanium and cobalt-chromium frameworks using five metal primers.
STATEMENT OF PROBLEM Poor chemical bonding of a denture base resin to cast titanium frameworks often introduces adhesive failure and increases microleakage. PURPOSE This study examined the shear bond strengths of a denture base resin to cast pure titanium, Ti-6Al-4V, and a cobalt-chromium alloy using various adhesive primers. MATERIAL AND METHODS Disks (6.0 mm diameter, 2.5 mm thick) were c...
متن کاملEffect of Primers on the Shear Bond Strength of Two Types of Acrylic Resin to Co-cr Partial Denture Alloy
The absence or poor chemical bonding of acrylic resin to Cobalt-Chromium metal frameworks, often introduces microleakage and bond failure at the interface. The aim of this study was to compare the shear bond strength of sandblasted cast and ingot cobaltchromium alloy to heat-cured and self-cured acrylic resins primed with four different metal primers. Fifty Co-Cr Ingot and fifty cast specimens ...
متن کاملEvaluation and comparison of the effect of different surface treatment modifications on the shear bond strength of a resin cement to titanium: An in vitro study
UNLABELLED The purpose of this study was to evaluate and compare the effect of grit blasting, chemical treatment, and application of alloy primer combinations on the shear bond strength (SBS) of a self-cure resin cement to titanium surface. MATERIALS AND METHODS Fifty cast commercially pure titanium discs (9 mm × 2 mm) were divided into five groups (n = 10), which received the following surfa...
متن کاملFactors affecting the bond strength of denture base and reline acrylic resins to base metal materials
OBJECTIVE The shear bond strengths of two hard chairside reline resin materials and an auto-polymerizing denture base resin material to cast Ti and a Co-Cr alloy treated using four conditioning methods were investigated. MATERIAL AND METHODS Disk specimens (diameter 10 mm and thickness 2.5 mm) were cast from pure Ti and Co-Cr alloy. The specimens were wet-ground to a final surface finish of 6...