Two-body and three-body abrasive wear behaviour of polyaryletherketone composites
نویسنده
چکیده
Single and multipass two-body and three-body abrasive wear behaviour of various polyaryletherketone composites have been carried out by using a pin-on-disc machine and a rubber wheel abrasion test (RWAT) rig. Abrasive wear studies were conducted under different loads and sliding distances. Comparative wear performance of all the composites at different loads shows that specific wear rate (Ko) of two-body abrasive wear (single pass condition) is 30-50 times greater than three-body abrasive wear. Also, specific wear rate (Ko) of two-body abrasive wear (multipass condition) is 5-12 times greater than three-body abrasive wear. Efforts were made to correlate the abrasive wear performance with the appropriate mechanical properties. The operating wear mechanisms under different experimental condition have also been studied by using scanning electron microscopy.
منابع مشابه
Three-body wear of different composites resins
Introduction: Low resistance of composite resins to abrasion is a primary concern in the application of these materials for posterior restorations which are prone to high occlusal loads. This study compared the wear resistance of three types of composites. Methods: In this laboratory experiment, five specimens of each of the three types of composites (z250, Heliomolar, Opallis) were prepared...
متن کاملبررسی اثر نوع فیلر بر سایش سه جزئی کامپوزیت دندانی
Statement of Problem: The relatively poor wear resistance of dental composite in stress bearing posterior situations has restricted wider clinical application of this restorative material. Purpose: The aim of this study was to evaluate the three body abrasive wear of a dental composite based on a new filler (leucite: KAl Si2O6) and to compare it with the wear resistance of a composite based on ...
متن کاملWear of composites by abrasives of varying hardness.
The relationship between the wear of three composite resins and the hardness of the abrasive was studied by a two-body abrasion test. The wear rates of the composites increased linearly with abrasive hardness from 530 to 2080 KHN. Measurement of the slope of the wear rate versus abrasive hardness over this range provided a sensitive method for ranking the composites.
متن کاملAbrasive Wear in Three-phase Waste-based Polymeric Particle Composites
Original scientific paper The experiment centres on two and three body abrasion in three-phase waste-based composite systems. The composite systems abrasion resistance is defined not only by the physical-mechanical relationships of the separate phases of the composite, but also by the mutual interaction of the phases and on the matrix-filler interface. To describe the composite system abrasion ...
متن کاملParametric optimization of Three-Body Abrasive Wear Behavior of Bidirectional and Short Kevlar Fiber Reinforced Epoxy Composites
In this article, the mechanical and three body abrasive wear behavior of Bidirectional and short Kevlar fiber reinforced epoxy composites at five different fiber loading (10wt%, 20wt%, 30wt%, 40wt% and 50wt%) have been evaluated. The mechanical properties i.e. tensile strength, flexural strength, inter-laminar-shear strength, and impact strength are performed to notice the behavior of mechanica...
متن کامل