Lithiation of individual silicon nanoparticles was studied in real time with in situ transmission electron microscopy. A strong size dependence of fracture was discovered; that is, there exists a critical particle diameter of ∼150 nm, below which the particles neither cracked nor fractured upon first lithiation, and above which the particles initially formed surface cracks and then fractured due to lithiation-induced swelling. The unexpected surface cracking arose owing to the buildup of large tensile hoop stress, which reversed the initial compression, in the surface layer. The stress reversal was attributed to the unique mechanism of lithiation in crystalline Si, taking place by movement of a two-phase boundary between the inner core of pristine Si and the outer shell of amorphous Li-Si alloy. While the resulting hoop tension tended to initiate surface cracks, the small-sized nanoparticles nevertheless averted fracture. This is because the stored strain energy from electrochemical reactions was insufficient to drive crack propagation, as dictated by the interplay between the two length scales, that is, particle diameter and crack size, that control the fracture. These results are diametrically opposite to those obtained previously from single-phase modeling, which predicted only compressive hoop stress in the surface layer and thus crack initiation from the center in lithiated Si particles and wires. Our work provides direct evidence of the mechanical robustness of small Si nanoparticles for applications in lithium ion batteries.
منابع مشابه
Tough germanium nanoparticles under electrochemical cycling.
Mechanical degradation of the electrode materials during electrochemical cycling remains a serious issue that critically limits the capacity retention and cyclability of rechargeable lithium-ion batteries. Here we report the highly reversible expansion and contraction of germanium nanoparticles under lithiation-delithiation cycling with in situ transmission electron microscopy (TEM). During mul...
متن کاملRobustness of amorphous silicon during the initial lithiation/delithiation cycle
Recent research on the electrochemical lithiation of amorphous silicon nanoparticles shows that amorphous silicon is more fracture resistant than crystalline silicon during lithiation. Nanoparticles of amorphous silicon can be lithiated and delithiated without any fracture at all. To fully exploit the potential of using amorphous silicon as electrodes for lithium ion batteries it is important t...
متن کاملPhase-field model for the two-phase lithiation of silicon
As an ideal anode material, silicon has the highest lithium-ion capacity in theory, but the broader application is limited by the huge volumetric strain caused by lithium insertion and extraction. To better understand the physical process and to resolve the related reliability issue, enormous efforts have been made. Recent experiments observed sharp reaction fronts in both crystalline and amorp...
متن کاملReaction Front Evolution during Electrochemical Lithiation of Crystalline Silicon Nanopillars
Silicon is one of the most promising anode materials for use in rechargeable lithium-ion batteries due to its high theoretical specific capacity of 4200 mAhg 1 and low cost. However, this high lithium storage capacity results in enormous volume expansion and contraction during electrochemical lithiation and delithiation, which can induce mechanical fracture and severe capacity fading. Recently,...
متن کاملIn Situ and Ex Situ TEM Study of Lithiation Behaviours of Porous Silicon Nanostructures
In this work, we study the lithiation behaviours of both porous silicon (Si) nanoparticles and porous Si nanowires by in situ and ex situ transmission electron microscopy (TEM) and compare them with solid Si nanoparticles and nanowires. The in situ TEM observation reveals that the critical fracture diameter of porous Si particles reaches up to 1.52 μm, which is much larger than the previously r...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- ACS nano
دوره 6 2 شماره
صفحات -
تاریخ انتشار 2012