Friction on a single MoS2 nanotube
نویسندگان
چکیده
Friction was measured on a single molybdenum disulfide (MoS2) nanotube and on a single MoS2 nano-onion for the first time. We used atomic force microscopy (AFM) operating in ultra-high vacuum at room temperature. The average coefficient of friction between the AFM tip and MoS2 nanotubes was found considerably below the corresponding values obtained from an air-cleaved MoS2 single crystal or graphite. We revealed a nontrivial dependency of friction on interaction strength between the nanotube and the underlying substrate. Friction on detached or weakly supported nanotubes by the substrate was several times smaller (0.023 ± 0.005) than that on well-supported nanotubes (0.08 ± 0.02). We propose an explanation of a quarter of a century old phenomena of higher friction found for intracrystalline (0.06) than for intercrystalline slip (0.025) in MoS2. Friction test on a single MoS2 nano-onion revealed a combined gliding-rolling process.PACS, 62.20, 61.46.Fg, 68.37 Ps.
منابع مشابه
Nanomechanical behavior of MoS2 and WS2 multi-walled nanotubes and Carbon nanohorns
Nano-objects have been investigated for drug delivery, oil detection, contaminant removal, and tribology applications. In some applications, they are subjected to friction and deformation during contact with each other and their surfaces on which they slide. Experimental studies directly comparing local and global deformation are lacking. This research performs nanoindentation (local deformatio...
متن کاملThe extended wedge method: atomic force microscope friction calibration for improved tolerance to instrument misalignments, tip offset, and blunt probes.
One of the major challenges in understanding and controlling friction is the difficulty in bridging the length and time scales of macroscale contacts and those of the single asperity interactions they comprise. While the atomic force microscope (AFM) offers a unique ability to probe tribological surfaces in a wear-free single-asperity contact, instrument calibration challenges have limited the ...
متن کاملThe tribological properties of Cu-Ni3Al-MoS2 composite coating deposited by magnetron sputtering
In industrial applications, most materials are exposed to wear and friction because multiple conditions are used. However, the tribological properties of these materials can be improved with different techniques. One such technique that improves the frictional property of a surface is the use of self-lubricating coatings. In this study, multicomponent coatings of nominal composition Cu-Ni3Al-Mo...
متن کاملTribological behavior of sputter-deposited MoSX/Ni coatings
AbstractSputtered MoS2 coatings have been mostly used as a solid lubricant. In this investigation, MoSx/Ni composite coatings with Ni contents varying from 0 to 22 % were deposited onto steel substrate using a DC magnetron sputter process. The MoS2/Ni ratio in the coatings was controlled by sputtering the composite targets. The composition, microstructure, and mechanical properties of the...
متن کاملStudy of tribological behavior of Cu–MoS2 and Ag–MoS2 nanocomposite lubricants
Tribological behavior of Cu-MoS2 and Ag-MoS2 nanocomposite lubricant was studied. Cu nanoparticles produced by electrical explosion of copper wires and Ag nanoparticles prepared by electrospark erosion were employed as metal cladding modifiers of MoS2 nanolamellar particles. The tribological tests showed Cu-MoS2 and Ag-MoS2 nanocomposite lubricants changed the friction coefficient of the initia...
متن کامل