Investigation on the Tribological Behavior and Wear Mechanism of Five Different Veneering Porcelains

نویسندگان

  • Jie Min
  • Qianqian Zhang
  • Xiaoli Qiu
  • Minhao Zhu
  • Haiyang Yu
  • Shanshan Gao
  • Jie Zheng
چکیده

OBJECTIVES The primary aim of this research was to investigate the wear behavior and wear mechanism of five different veneering porcelains. METHODS Five kinds of veneering porcelains were selected in this research. The surface microhardness of all the samples was measured with a microhardness tester. Wear tests were performed on a ball-on-flat PLINT fretting wear machine, with lubrication of artificial saliva at 37°C. The friction coefficients were recorded by the testing system. The microstructure features, wear volume, and damage morphologies were recorded and analyzed with a confocal laser scanning microscope and a scanning electron microscope. The wear mechanism was then elucidated. RESULTS The friction coefficients of the five veneering porcelains differ significantly. No significant correlation between hardness and wear volume was found for these veneering porcelains. Under lubrication of artificial saliva, the porcelain with higher leucite crystal content exhibited greater wear resistance. Additionally, leucite crystal size and distribution in glass matrix influenced wear behavior. The wear mechanisms for these porcelains were similar: abrasive wear dominates the early stage, whereas delamination was the main damage mode at the later stage. Furthermore, delamination was more prominent for porcelains with larger crystal sizes. SIGNIFICANCE Wear compatibility between porcelain and natural teeth is important for dental restorative materials. Investigation on crystal content, size, and distribution in glass matrix can provide insight for the selection of dental porcelains in clinical settings.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of Welding Parameters on the Room and High Temperature Tribological Behavior of the Weld Overlaid Die

As an important problem in forging factories, dies are destroyed because of high wear rate, plastic deformation and thermal and mechanical fatigue at high temperatures. This paper is an investigation into        the use of nickel super alloy with different welding parameters. Three weld overlaid alloys of inconel625, as wear resistance hardfacing materials on H13 tool steel, with different weld...

متن کامل

The Effect of Carbides Morphology on Tribological Behaviour of Ni-Hard 4 Cast Irons

In this research the effect of volume and morphology of eutectic carbides on tribological behaviour of Ni-Hard 4 cast irons have been investigated. Therefore, as a result of the fact that the carbon content effects the carbides morphology of Ni-hard cast irons, the chemical compositions of five different specimens were kept constant with the exception of the carbon content, which was varied fro...

متن کامل

The Effect of Carbides Morphology on Tribological Behaviour of Ni-Hard 4 Cast Irons

In this research the effect of volume and morphology of eutectic carbides on tribological behaviour of Ni-Hard 4 cast irons have been investigated. Therefore, as a result of the fact that the carbon content effects the carbides morphology of Ni-hard cast irons, the chemical compositions of five different specimens were kept constant with the exception of the carbon content, which was varied fro...

متن کامل

Investigation of Wear Behavior of Biopolymers for Total Knee Replacements Through Invitro Experimentation

The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR  is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...

متن کامل

Tribological behavior of sputter-deposited MoSX/Ni coatings

AbstractSputtered MoS2 coatings have been mostly used as a solid lubricant. In this investigation, MoSx/Ni composite coatings with Ni contents varying from 0 to 22 % were deposited onto steel substrate using a DC magnetron sputter process. The MoS2/Ni ratio in the coatings was controlled by sputtering the composite targets. The composition, microstructure, and mechanical properties of the...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 10  شماره 

صفحات  -

تاریخ انتشار 2015