Shear bond strengths of self-etching adhesives to caries-affected dentin on the gingival wall.

نویسندگان

  • Alp Erdin Koyuturk
  • Abdulkadir Sengun
  • Fusun Ozer
  • Yagmur Sener
  • Alparslan Gokalp
چکیده

The purpose of this study was to evaluate the bonding ability of five current self-etching adhesives to caries-affected dentin on the gingival wall. Seventy extracted human molars with approximal dentin caries were employed in this study. In order to obtain caries-affected dentin on the gingival wall, grinding was performed under running water. Following which, specimens mounted in acrylic blocks and composite resins of the bonding systems were bonded to dentin with plastic rings and then debonded by shear bond strength. With Clearfil SE Bond, bonding to caries-affected dentin showed the highest bond strength. With Optibond Solo Plus Self-Etch, bonding to caries-affected dentin showed higher shear bond strength than AQ Bond, Tyrian SPE & One-Step Plus, and Prompt-L-Pop (p<0.05). Further, the bond strengths of Clearfil SE Bond and Optibond Solo Plus Self-Etch to sound dentin were higher than those of Prompt-L-Pop, AQ Bond, and Tyrian SPE & One-Step Plus (p<0.05). In conclusion, besides micromechanical interlocking through hybrid layer formation, bond strength of self-etch adhesives to dentin may be increased from additional chemical interaction between the functional monomer and residual hydroxyapatite. The results of this study confirmed that differences in bond strength among self-etching adhesives to both caries-affected and sound dentin were due to chemical composition rather than acidity.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Bonding of self-etch and total-etch adhesives to carious dentin.

Carious dentin is partially demineralized and contains mineral crystals in the tubules. This may permit the deeper etching of intertubular dentin but prevent resin tag formation during bonding. We hypothesize that resin adhesives will produce lower bond strengths to caries-infected and caries-affected dentin compared with normal dentin. We tested this by measuring the microtensile bond strength...

متن کامل

Dentin wetting by four adhesive systems.

OBJECTIVES To evaluate the dentin wetting by four adhesive systems and to relate the wetting properties with the adhesive efficiency. METHODS Scotch Bond Multipurpose Plus (3M), Syntac Single-Component (Vivadent), One-Step (Bisco) and Heliobond (Vivadent) were used. The substrate was superficial and deep human dentin. Roughness and water contact angle were measured before and after acid etchi...

متن کامل

Microtensile bond strength of total-etch and self-etching adhesives to caries-affected dentine.

OBJECTIVES To evaluate the microtensile bond strength of total-etch or self-etch adhesives to caries-affected versus normal dentine, and to correlate these bond strengths with DIAGNOdent laser fluorescence and Knoop microhardness (KH) measurements of the substrates. METHODS Extracted carious human molars were ground to expose flat surfaces where the caries lesion was surrounded by normal dent...

متن کامل

Shear bond strength of different adhesive systems to normal and caries-affected dentin

BACKGROUND AND AIM: According to the effect of the adhesive and substrate type on the bond strength, examination of the adhesive is required in all aspects. The aim of this study was to evaluate the shear bond strength of different adhesive systems to normal dentin (ND) and caries affected dentin (CAD) in permanent teeth. METHODS: Thirty extracted molars with small occlusal caries were selected...

متن کامل

Effect of Chlorhexidine on Micro-Shear Bond Strength of Two Adhesive Systems After Aging

Background and Aim: Recurrent caries and low bond strength are the main causes of composite restorations failure. This study sought to assess the effect of chlorhexidine (CHX) on micro-shear bond strength (MSBS) to dentin of a fourth generation adhesive system and a universal bonding agent after aging. Materials and Methods: This in vitro study used 32 extracted third molars and 3-5mm thick de...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Dental materials journal

دوره 25 1  شماره 

صفحات  -

تاریخ انتشار 2006